A Hygroscopic Composite Backplate Enabling Passive Cooling of Photovoltaic Panels AITranslate

Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cooling photovoltaics (PV) matters since elevated temperature reduces efficiency and lifetime, but it is a great challenge when simultaneously pursuing effective cooling, low material cost, and light extra components. We herein propose a composite backplate for the passive cooling of PV panels, which consists of hygroscopic hydrogels with an adsorption-evaporative cooling effect and protective membranes. Besides, instant tough bonding with conventional PV backsheet allows for the composite backplate ease of implementation. Consequently, the composite backplate demonstrates nondegrading cooling performance during multiday field tests. Compared to a normal PV panel with good ventilation conditions, the average temperature reduction of each day varies from 1.5 to 6.4 °C under different climate conditions, indicating the absolute energy yield would increase by 0.57% to 2.43% of the yield under 25 °C. Considering the nearly unchanged appearance, moderate weight increase, and low raw material costs, this composite backplate facilitates benefiting from cooling PV panels attainable.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00196

Chinese Library Classification Number:

Citation Information:

Cooling photovoltaics (PV) matters since elevated temperature reduces efficiency and lifetime, but it is a great challenge when simultaneously pursuing effective cooling, low material cost, and light extra components. We herein propose a composite backplate for the passive cooling of PV panels, which consists of hygroscopic hydrogels with an adsorption-evaporative cooling effect and protective membranes. Besides, instant tough bonding with conventional PV backsheet allows for the composite backplate ease of implementation. Consequently, the composite backplate demonstrates nondegrading cooling performance during multiday field tests. Compared to a normal PV panel with good ventilation conditions, the average temperature reduction of each day varies from 1.5 to 6.4 °C under different climate conditions, indicating the absolute energy yield would increase by 0.57% to 2.43% of the yield under 25 °C. Considering the nearly unchanged appearance, moderate weight increase, and low raw material costs, this composite backplate facilitates benefiting from cooling PV panels attainable.

quote

GB/T 7714-2015 [1] Zhenpeng Li, Tao Ma, Fan Ji, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00196.
MLA [1] Zhenpeng Li, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00196.
APA [1] Zhenpeng Li, Tao Ma, Fan Ji, He Shan, Yanjun Dai, & Ruzhu Wang. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00196
IEEE [1] Zhenpeng Li, Tao Ma, Fan Ji, He Shan, Yanjun Dai, and Ruzhu Wang, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00196.