Photothermal Supercapacitors with Gel Polymer Electrolytes for Wide Temperature Range Operation AITranslate

University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To deliver electrochemical energy over a wide range of temperatures, this work studies a new gel polymer electrolyte (GPE) for photothermal supercapacitors operating from −60 to 65 °C. The GPE consists of polyacrylonitrile mixed with an active filler sodium polystyrenesulfonate that simultaneously improves ionic conductivity and traps metal cation impurities. The self-discharge rate and impurity diffusion coefficients in the supercapacitors were lowered by the active filler to minimize energy loss in hot environments. For cold settings, the devices were packaged with a photothermal conversion layer that increased the internal cell temperature and raised the energy density to 94 μWh/cm2 at the output power density of 0.4 mW/cm2 in a −60 °C chamber. The combination of our improved GPE and photothermal conversion increased the stored energy and thereby extended the operational time of a motor driven from a cold start by a supercapacitor, demonstrating a high-performance design suitable for harsh environments.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00207

Chinese Library Classification Number:

Citation Information:

To deliver electrochemical energy over a wide range of temperatures, this work studies a new gel polymer electrolyte (GPE) for photothermal supercapacitors operating from −60 to 65 °C. The GPE consists of polyacrylonitrile mixed with an active filler sodium polystyrenesulfonate that simultaneously improves ionic conductivity and traps metal cation impurities. The self-discharge rate and impurity diffusion coefficients in the supercapacitors were lowered by the active filler to minimize energy loss in hot environments. For cold settings, the devices were packaged with a photothermal conversion layer that increased the internal cell temperature and raised the energy density to 94 μWh/cm2 at the output power density of 0.4 mW/cm2 in a −60 °C chamber. The combination of our improved GPE and photothermal conversion increased the stored energy and thereby extended the operational time of a motor driven from a cold start by a supercapacitor, demonstrating a high-performance design suitable for harsh environments.

quote

GB/T 7714-2015 [1] Chanho Shin, Lulu Yao, Haichen Lin, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00207.
MLA [1] Chanho Shin, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00207.
APA [1] Chanho Shin, Lulu Yao, Haichen Lin, Ping Liu, & Tse Nga Ng. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00207
IEEE [1] Chanho Shin, Lulu Yao, Haichen Lin, Ping Liu, and Tse Nga Ng, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00207.