Dual Ligand Capped Quantum Dots Improving Loading Amount for High-Efficiency Quantum Dot-Sensitized Solar Cells AITranslate

South China Agricultural University; South China Agricultural University; South China Agricultural University; South China Agricultural University; South China Agricultural University; South China Agricultural University; South China Agricultural University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In quantum dot sensitized solar cells (QDSCs), high loading of high-quality QD sensitizers is a prerequisite for high photovoltaic performance. Herein, a facile and effective ligand design strategy to improve both the loading amount and optoelectronic performance of QD sensitizers is developed by decorating the QD surface with dual ligands of mercaptopropionic acid (MPA) and inorganic ligands (ILs). Experimental results demonstrate that the coexistence of ILs with MPA can not only reduce solvation energy that facilitates QD loading but also serve as effective cross-linkers for the reduction of interdot repulsion and formation of dense QD layers. Furthermore, various ILs, represented by pseudohalide SCN–, exhibit a great passivation effect on QD surfaces and suppress the defect trap states. Due to these benefits, Zn–Cu–In–S–Se (ZCISSe) QDSCs based on dual SCN/MPA ligands deliver a certified efficiency of 16.10%, which is a new record efficiency for liquid-junction QD solar cells.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02270

Chinese Library Classification Number:

Citation Information:

In quantum dot sensitized solar cells (QDSCs), high loading of high-quality QD sensitizers is a prerequisite for high photovoltaic performance. Herein, a facile and effective ligand design strategy to improve both the loading amount and optoelectronic performance of QD sensitizers is developed by decorating the QD surface with dual ligands of mercaptopropionic acid (MPA) and inorganic ligands (ILs). Experimental results demonstrate that the coexistence of ILs with MPA can not only reduce solvation energy that facilitates QD loading but also serve as effective cross-linkers for the reduction of interdot repulsion and formation of dense QD layers. Furthermore, various ILs, represented by pseudohalide SCN–, exhibit a great passivation effect on QD surfaces and suppress the defect trap states. Due to these benefits, Zn–Cu–In–S–Se (ZCISSe) QDSCs based on dual SCN/MPA ligands deliver a certified efficiency of 16.10%, which is a new record efficiency for liquid-junction QD solar cells.

quote

GB/T 7714-2015 [1] Zhengyan Zhang, Han Song, Wenran Wang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02270.
MLA [1] Zhengyan Zhang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02270.
APA [1] Zhengyan Zhang, Han Song, Wenran Wang, Huashang Rao, Yueping Fang, Zhenxiao Pan, & Xinhua Zhong. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02270
IEEE [1] Zhengyan Zhang, Han Song, Wenran Wang, Huashang Rao, Yueping Fang, Zhenxiao Pan, and Xinhua Zhong, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02270.