Enhancing Tensile Strength and Toughness via Moderate Orientation of Amorphous Molecular Chains in Biobased Biodegradable Poly(lactic acid) AITranslate

South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology;Tianjin Institute of Industrial Biotechnology; Guangxi University of Science and Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The preparation of high-toughness and high-strength poly(lactic acid) (PLA) is of great significance for promoting its application in packing, construction, and medical fields. Compared to blending with polymeric elastomers, hot stretching is an effective method to improve the toughness of PLA without sacrificing its strength. However, it is still unclear which part of the structural change after hot stretching is responsible for the increased toughness of PLA. In this work, the semicrystalline structure and mechanical properties of the PLA samples stretched at different temperatures were studied. First, the semicrystalline structure of the PLA samples was studied by combining differential scanning calorimetry and wide-angle X-ray diffraction analyses. When the stretching temperature was relatively low (e.g., 65 °C), the mesophase, an intermediate phase between crystal and amorphous, was formed. Furthermore, significant stretch-induced crystallization was observed due to the enhanced chain mobility when the stretching temperature was 65–75 °C. With further increasing the stretching temperature, the crystallinity of the PLA samples decreased sharply to nearly 0 due to the rapid chain relaxation. Intriguingly, the PLA samples stretched at 85 °C showed the highest elongation at break 238.4% and high strength 75.8 MPa, which was attributed to its moderate molecular chain orientation not only hindering physical aging but also retaining the entanglement network of PLA molecular chains. The findings in this work provide an insightful understanding of the improved toughness of PLA, which will facilitate the large-scale practical application of PLA.

KeyWords AITranslate

poly(lactic acid) hot stretching semicrystalline structure enhanced mechanical properties orientation of amorphous
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00898

Chinese Library Classification Number:

Citation Information:

The preparation of high-toughness and high-strength poly(lactic acid) (PLA) is of great significance for promoting its application in packing, construction, and medical fields. Compared to blending with polymeric elastomers, hot stretching is an effective method to improve the toughness of PLA without sacrificing its strength. However, it is still unclear which part of the structural change after hot stretching is responsible for the increased toughness of PLA. In this work, the semicrystalline structure and mechanical properties of the PLA samples stretched at different temperatures were studied. First, the semicrystalline structure of the PLA samples was studied by combining differential scanning calorimetry and wide-angle X-ray diffraction analyses. When the stretching temperature was relatively low (e.g., 65 °C), the mesophase, an intermediate phase between crystal and amorphous, was formed. Furthermore, significant stretch-induced crystallization was observed due to the enhanced chain mobility when the stretching temperature was 65–75 °C. With further increasing the stretching temperature, the crystallinity of the PLA samples decreased sharply to nearly 0 due to the rapid chain relaxation. Intriguingly, the PLA samples stretched at 85 °C showed the highest elongation at break 238.4% and high strength 75.8 MPa, which was attributed to its moderate molecular chain orientation not only hindering physical aging but also retaining the entanglement network of PLA molecular chains. The findings in this work provide an insightful understanding of the improved toughness of PLA, which will facilitate the large-scale practical application of PLA.

quote

GB/T 7714-2015 [1] Jiqian Li, Mohong Xu, Hezhi He, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00898.
MLA [1] Jiqian Li, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00898.
APA [1] Jiqian Li, Mohong Xu, Hezhi He, Qi Gao, Yiming Zhang, He Zhang, Qun Gu, Bin Xue, & Zhiwen Zhu. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00898
IEEE [1] Jiqian Li, Mohong Xu, Hezhi He, Qi Gao, Yiming Zhang, He Zhang, Qun Gu, Bin Xue, and Zhiwen Zhu, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00898. keywords: {poly(lactic acid);hot stretching;semicrystalline structure;enhanced mechanical properties;orientation of amorphous}