Optimization of the Thermoelectric Properties of 2D-PEDOT Derivative Chains Using Electrochemical Control AITranslate

Gachon University; University of Chicago
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Conductive organic-based thermoelectric generators are very effective in collecting electricity from waste heat with low-temperature gradients compared to ambient conditions. Although studies have been conducted to improve thermoelectric characteristics by doping conducting polymers, the thermoelectric performances achieved by accurately controlling the doping level of polymer chains are currently inadequate. Here, we report changes in thermoelectric performance of three-armed cross-linker introduced poly(3,4-ethylenedioxythiophene) (PEDOT) derivative two-dimensional (2D) chain using electrochemical oxidation level control. The charge carrier density of PEDOT derivative films increased with more positive potentials (from 0.7 × 1020 to 4.24 × 1021) and was precisely controlled by varying potentials. Thermoelectric properties such as electrical conductivity, carrier mobility, and Seebeck coefficients were also manipulated through the application of different potentials. The power factor of the PEDOT derivative 2D chain was improved to 72.6 μW m–1 K–2 at +0.6 V, which was much higher than that of a neutral state at −1.4 V (5.1 × 10–2 μW m–1 K–2).

KeyWords AITranslate

organic thermoelectric poly(3 4ethylenedioxythiophene) doping control electrical conductivity Seebeck coefficient
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00899

Chinese Library Classification Number:

Citation Information:

Conductive organic-based thermoelectric generators are very effective in collecting electricity from waste heat with low-temperature gradients compared to ambient conditions. Although studies have been conducted to improve thermoelectric characteristics by doping conducting polymers, the thermoelectric performances achieved by accurately controlling the doping level of polymer chains are currently inadequate. Here, we report changes in thermoelectric performance of three-armed cross-linker introduced poly(3,4-ethylenedioxythiophene) (PEDOT) derivative two-dimensional (2D) chain using electrochemical oxidation level control. The charge carrier density of PEDOT derivative films increased with more positive potentials (from 0.7 × 1020 to 4.24 × 1021) and was precisely controlled by varying potentials. Thermoelectric properties such as electrical conductivity, carrier mobility, and Seebeck coefficients were also manipulated through the application of different potentials. The power factor of the PEDOT derivative 2D chain was improved to 72.6 μW m–1 K–2 at +0.6 V, which was much higher than that of a neutral state at −1.4 V (5.1 × 10–2 μW m–1 K–2).

quote

GB/T 7714-2015 [1] Jun Seop Lee, Shrayesh N. Patel. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00899.
MLA [1] Jun Seop Lee, and Shrayesh N. Patel. ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00899.
APA [1] Jun Seop Lee, & Shrayesh N. Patel. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00899
IEEE [1] Jun Seop Lee and Shrayesh N. Patel, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00899. keywords: {organic thermoelectric;poly(3;4ethylenedioxythiophene);doping control;electrical conductivity;Seebeck coefficient}