daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

High-Performance Quasi-Solid-State Flexible Aqueous Rechargeable Ag–Zn Battery Based on Metal–Organic Framework-Derived Ag Nanowires AITranslate

University of Science and Technology of China; Suzhou Institute of Nano-tech and Nano-bionics; Suzhou Institute of Nano-tech and Nano-bionics; Nanjing University; Nanjing University; Suzhou Institute of Nano-tech and Nano-bionics; Suzhou Institute of Nano-tech and Nano-bionics; Suzhou Institute of Nano-tech and Nano-bionics; Suzhou Institute of Nano-tech and Nano-bionics; Nanjing University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Silver–zinc (Ag–Zn) batteries are one of the promising aqueous batteries to collect and store solar energy with high energy density, a stable output voltage, and being environmentally benign, but most Ag–Zn batteries have large contact resistance caused by polymer binders and conductive additives, thus leading to their low specific capacity and rate performance. As a proof-of-concept demonstration, we constructed a solar charged planar flexible quasi-solid-state aqueous rechargeable Ag–Zn battery using metal–organic framework (MOF)-derived Ag nanowires on carbon cloth as a binder-free cathode. Our electrochemical results show that the as-fabricated Ag–Zn battery has a remarkable energy density of 1.87 mWh/cm2 because MOF-derived Ag nanowires can provide abundant reaction sites and short electron and ion diffusion paths. Moreover, the as-fabricated Ag–Zn battery integrated with a solar cell can be charged by sunlight. Thus, our findings pave an avenue to develop solar energy-powered portable and wearable electronic devices.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01675

Chinese Library Classification Number:

Citation Information:

Silver–zinc (Ag–Zn) batteries are one of the promising aqueous batteries to collect and store solar energy with high energy density, a stable output voltage, and being environmentally benign, but most Ag–Zn batteries have large contact resistance caused by polymer binders and conductive additives, thus leading to their low specific capacity and rate performance. As a proof-of-concept demonstration, we constructed a solar charged planar flexible quasi-solid-state aqueous rechargeable Ag–Zn battery using metal–organic framework (MOF)-derived Ag nanowires on carbon cloth as a binder-free cathode. Our electrochemical results show that the as-fabricated Ag–Zn battery has a remarkable energy density of 1.87 mWh/cm2 because MOF-derived Ag nanowires can provide abundant reaction sites and short electron and ion diffusion paths. Moreover, the as-fabricated Ag–Zn battery integrated with a solar cell can be charged by sunlight. Thus, our findings pave an avenue to develop solar energy-powered portable and wearable electronic devices.

quote

GB/T 7714-2015 [1] Chaowei Li, Qichong Zhang, Juan Sun, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01675.
MLA [1] Chaowei Li, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01675.
APA [1] Chaowei Li, Qichong Zhang, Juan Sun, Taotao Li, Songfeng E, Zezhou Zhu, Bing He, Zhenyu Zhou, Qiulong Li, & Yagang Yao. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01675
IEEE [1] Chaowei Li, Qichong Zhang, Juan Sun, Taotao Li, Songfeng E, Zezhou Zhu, Bing He, Zhenyu Zhou, Qiulong Li, and Yagang Yao, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01675.