Yin-Yang Harmony: Metal and Nonmetal Dual-Doping Boosts Electrocatalytic Activity for Alkaline Hydrogen Evolution AITranslate
Abstract AITranslate
Active site number, water dissociation, and hydrogen adsorption free energy are the three main parameters for regulating the activity of electrocatalysts for hydrogen evolution reaction (HER) in alkaline media. However, at present, simultaneous modulations of these three parameters for alkaline HER still remain challenging. In this work, we take CoP as the model material and demonstrate that a metal and nonmetal dual-doping strategy can achieve simultaneous modulation of these three parameters by inducing lattice irregularity and optimizing the electronic configuration in CoP nanomaterials. Benefiting from the oxygen and copper dual-doping collective effect, the optimized O,Cu–CoP nanowire array electrode shows nearly 10-fold enhancement in catalytic activity for alkaline HER compared to a pure CoP nanowire electrode. Our work may provide a new concept to boost performance of nonprecious metal electrocatalysts for alkaline HER.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b01893
Chinese Library Classification Number:
Citation Information:
Active site number, water dissociation, and hydrogen adsorption free energy are the three main parameters for regulating the activity of electrocatalysts for hydrogen evolution reaction (HER) in alkaline media. However, at present, simultaneous modulations of these three parameters for alkaline HER still remain challenging. In this work, we take CoP as the model material and demonstrate that a metal and nonmetal dual-doping strategy can achieve simultaneous modulation of these three parameters by inducing lattice irregularity and optimizing the electronic configuration in CoP nanomaterials. Benefiting from the oxygen and copper dual-doping collective effect, the optimized O,Cu–CoP nanowire array electrode shows nearly 10-fold enhancement in catalytic activity for alkaline HER compared to a pure CoP nanowire electrode. Our work may provide a new concept to boost performance of nonprecious metal electrocatalysts for alkaline HER.
quote
| GB/T 7714-2015 | [1] Kun Xu, Yiqiang Sun, Yuanmiao Sun, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01893. |
| MLA | [1] Kun Xu, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01893. |
| APA | [1] Kun Xu, Yiqiang Sun, Yuanmiao Sun, Yongqi Zhang, Guichong Jia, Qinghua Zhang, Lin Gu, Shuzhou Li, Yue Li, & Hong Jin Fan. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01893 |
| IEEE | [1] Kun Xu, Yiqiang Sun, Yuanmiao Sun, Yongqi Zhang, Guichong Jia, Qinghua Zhang, Lin Gu, Shuzhou Li, Yue Li, and Hong Jin Fan, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01893. |