daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

One-part slag/zeolite geopolymer mortars under ambient and heat curing conditions AITranslate

Østfold University College; Islamic Azad University; Islamic Azad University; Islamic Azad University;School of Housing, Building and Planning; Østfold University College
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Geopolymer materials can be formulated with a variety of precursors rich in aluminosilicates. However, some of these precursors, which are industrial by-products, are not widely available in the world. Therefore, there is a need to explore alternative potential precursors derived from natural sources. This study investigates the viability of using natural zeolite utilization as a part of the precursor in one-part ground granulated blast furnace slag (GGBFS)-based geopolymer mortars activated with sodium metasilicate. Geopolymer mortars were made with 0–90 wt% natural zeolite and cured at ambient and 40 ℃ temperatures. Fresh and hardened properties were evaluated. The test results showed that zeolite addition reduced the workability and setting time of the fresh mortar, significantly. Furthermore, the mechanical strength dropped with increasing zeolite content due to the microporous structure of the zeolite particles and weak reaction products. The microstructural examination showed that the mortars containing zeolite had a more porous structure compared to the pure slag mortar. Furthermore, heat-curing increased the mechanical strength in all mortars and densified the microstructure.

KeyWords AITranslate

Onepart geopolymer Natural zeolite GGBFS Heatcuring Mechanical strength
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2023.e02677

Chinese Library Classification Number:

Citation Information:

Geopolymer materials can be formulated with a variety of precursors rich in aluminosilicates. However, some of these precursors, which are industrial by-products, are not widely available in the world. Therefore, there is a need to explore alternative potential precursors derived from natural sources. This study investigates the viability of using natural zeolite utilization as a part of the precursor in one-part ground granulated blast furnace slag (GGBFS)-based geopolymer mortars activated with sodium metasilicate. Geopolymer mortars were made with 0–90 wt% natural zeolite and cured at ambient and 40 ℃ temperatures. Fresh and hardened properties were evaluated. The test results showed that zeolite addition reduced the workability and setting time of the fresh mortar, significantly. Furthermore, the mechanical strength dropped with increasing zeolite content due to the microporous structure of the zeolite particles and weak reaction products. The microstructural examination showed that the mortars containing zeolite had a more porous structure compared to the pure slag mortar. Furthermore, heat-curing increased the mechanical strength in all mortars and densified the microstructure.

quote

GB/T 7714-2015 [1] Parham Shoaei, Abazar Momenzadeh, Hamed Hosseini, et al. Case Studies in Construction Materials, 2024(20). DOI:10.1016/j.cscm.2023.e02677.
MLA [1] Parham Shoaei, et al., Case Studies in Construction Materials, no. 20, 2024, https://doi.org/10.1016/j.cscm.2023.e02677.
APA [1] Parham Shoaei, Abazar Momenzadeh, Hamed Hosseini, Shahin Rajaei, Farshad Ameri, & Shima Pilehvar. (2024). Case Studies in Construction Materials(20). https://doi.org/10.1016/j.cscm.2023.e02677
IEEE [1] Parham Shoaei, Abazar Momenzadeh, Hamed Hosseini, Shahin Rajaei, Farshad Ameri, and Shima Pilehvar, Case Studies in Construction Materials, no. 20, 2024, doi: 10.1016/j.cscm.2023.e02677. keywords: {Onepart geopolymer;Natural zeolite;GGBFS;Heatcuring;Mechanical strength}