In Vitro Osteosarcoma Models Based on 3D-Printed Composite Scaffolds to Reveal Cellular Responses, Molecular Mechanisms and Predictive Biomarkers AITranslate
Abstract AITranslate
Osteosarcoma (OS) is the most diagnosed bone tumor in children, and current in vitro methods (2D cell culture and tumor spheroids) cannot appropriately reflect the real extracellular matrix of OS. Here, three subtypes of in vitro OS models were fabricated based on 3D-printed composite scaffolds consisting of hydroxyapatite and β-tricalcium phosphate with different ratios. The phenotypes of cell proliferation, morphology, migration, and epithelial-mesenchymal transition progression were investigated. Compared with ordinary methods, the scaffold-based OS models obtained the obvious advantage of inducing fatty acid biosynthesis, synthase expression, and classic signaling pathway. The metabolomic analysis revealed that the most abundant metabolites appeared in the type of lipids, and the metabolic differences mainly came from biosynthesis of unsaturated fatty acids. The comparison with clinical trials indicated the scaffold-based model as a potential alternative platform to discover OS pathogenesis mechanisms and to develop novel diagnosis methods that would be otherwise missed in ordinary ways.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.3c01049
Chinese Library Classification Number:
Citation Information:
Osteosarcoma (OS) is the most diagnosed bone tumor in children, and current in vitro methods (2D cell culture and tumor spheroids) cannot appropriately reflect the real extracellular matrix of OS. Here, three subtypes of in vitro OS models were fabricated based on 3D-printed composite scaffolds consisting of hydroxyapatite and β-tricalcium phosphate with different ratios. The phenotypes of cell proliferation, morphology, migration, and epithelial-mesenchymal transition progression were investigated. Compared with ordinary methods, the scaffold-based OS models obtained the obvious advantage of inducing fatty acid biosynthesis, synthase expression, and classic signaling pathway. The metabolomic analysis revealed that the most abundant metabolites appeared in the type of lipids, and the metabolic differences mainly came from biosynthesis of unsaturated fatty acids. The comparison with clinical trials indicated the scaffold-based model as a potential alternative platform to discover OS pathogenesis mechanisms and to develop novel diagnosis methods that would be otherwise missed in ordinary ways.
quote
| GB/T 7714-2015 | [1] MeiLing Wang, XueYu Chen, NianYuan Xu, et al. ACS Materials Letters, 2024(6). DOI:10.1021/acsmaterialslett.3c01049. |
| MLA | [1] MeiLing Wang, et al., ACS Materials Letters, no. 6, 2024, https://doi.org/10.1021/acsmaterialslett.3c01049. |
| APA | [1] MeiLing Wang, XueYu Chen, NianYuan Xu, Jun Li, Ruizhi Tang, & XiQiu Liu. (2024). ACS Materials Letters(6). https://doi.org/10.1021/acsmaterialslett.3c01049 |
| IEEE | [1] MeiLing Wang, XueYu Chen, NianYuan Xu, Jun Li, Ruizhi Tang, and XiQiu Liu, ACS Materials Letters, no. 6, 2024, doi: 10.1021/acsmaterialslett.3c01049. |