Heterostructure CsPbBr3/SrBrF Nanocrystals Stabilize Perovskite LEDs with Suppressed Halogen Ion Migration AITranslate
Abstract AITranslate
Ion migration is a fundamental problem for perovskite nanocrystal-based light-emitting diodes (PNC-LEDs)─a forerunner in next-generation displays and lighting technologies. Here, we report on monodisperse heterostructure CsPbBr3 perovskite nanocrystals capped with satellite SrBrF nanocrystals for stabilized and improved PNC-LEDs. We show that capping SrBrF can passivate surface carrier traps and improve the photoluminescence quantum yields of CsPbBr3 nanocrystals from 43.3% to 89.0%, showing about a 28-fold improvement in thermal stability (at 363 K) and exceptional photostability under long-term ultraviolet exposure (at 365 nm). The fabricated PNC-LEDs show significantly improved external quantum efficiency (EQE) (18.5%, 80-fold higher), maximum luminance (1604 cd/m2, 3-fold higher), and half-life (28 min, 14-fold higher), compared with the one fabricated with unmodified CsPbBr3 nanocrystals. Time-of-flight secondary-ion mass spectrometry (TOF-SIMS) studies gave compelling evidence of inhibited halogen ion migration in CsPbBr3/SrBrF PNC-LEDs due to the capping of SrBrF nanocrystals. This approach has important implications for fabricating high-performance PNC-LEDs with suppressed halogen ion migration.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.3c01176
Chinese Library Classification Number:
Citation Information:
Ion migration is a fundamental problem for perovskite nanocrystal-based light-emitting diodes (PNC-LEDs)─a forerunner in next-generation displays and lighting technologies. Here, we report on monodisperse heterostructure CsPbBr3 perovskite nanocrystals capped with satellite SrBrF nanocrystals for stabilized and improved PNC-LEDs. We show that capping SrBrF can passivate surface carrier traps and improve the photoluminescence quantum yields of CsPbBr3 nanocrystals from 43.3% to 89.0%, showing about a 28-fold improvement in thermal stability (at 363 K) and exceptional photostability under long-term ultraviolet exposure (at 365 nm). The fabricated PNC-LEDs show significantly improved external quantum efficiency (EQE) (18.5%, 80-fold higher), maximum luminance (1604 cd/m2, 3-fold higher), and half-life (28 min, 14-fold higher), compared with the one fabricated with unmodified CsPbBr3 nanocrystals. Time-of-flight secondary-ion mass spectrometry (TOF-SIMS) studies gave compelling evidence of inhibited halogen ion migration in CsPbBr3/SrBrF PNC-LEDs due to the capping of SrBrF nanocrystals. This approach has important implications for fabricating high-performance PNC-LEDs with suppressed halogen ion migration.
quote
| GB/T 7714-2015 | [1] Hujiabudula Maimaitizi, Deyang Li, Abulikemu Abulizi, et al. ACS Materials Letters, 2024(6). DOI:10.1021/acsmaterialslett.3c01176. |
| MLA | [1] Hujiabudula Maimaitizi, et al., ACS Materials Letters, no. 6, 2024, https://doi.org/10.1021/acsmaterialslett.3c01176. |
| APA | [1] Hujiabudula Maimaitizi, Deyang Li, Abulikemu Abulizi, Saiyaremu Halifu, Tengling Ye, & Guanying Chen. (2024). ACS Materials Letters(6). https://doi.org/10.1021/acsmaterialslett.3c01176 |
| IEEE | [1] Hujiabudula Maimaitizi, Deyang Li, Abulikemu Abulizi, Saiyaremu Halifu, Tengling Ye, and Guanying Chen, ACS Materials Letters, no. 6, 2024, doi: 10.1021/acsmaterialslett.3c01176. |