daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Vacuum-Deposited 2D/3D Perovskite Heterojunctions AITranslate

Universidad de Valencia;Helmholtz-Zentrum Berlin für Materialien und Energie GmbH, Young Investigator Group for Perovskite Tandem Solar Cells; Delft University of Technology; Universidad de Valencia; Delft University of Technology; Universidad de Valencia; Universidad de Valencia
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Low-dimensional (quasi-) 2D perovskites are being extensively studied in order to enhance the stability and the open-circuit voltage of perovskite solar cells. Up to now, thin 2D perovskite layers on the surface and/or at the grain boundaries of 3D perovskites have been deposited solely by solution processing, leading to unavoidable intermixing between the two phases. In this work, we report the fabrication of 2D/3D/2D perovskite heterostructures by dual-source vacuum deposition, with the aim of studying the interaction between the 3D and 2D phases as well as the charge transport properties of 2D perovskites in neat 2D/3D interfaces. Unlike what is normally observed in solution-processed 3D/2D systems, we found a reduced charge transport with no direct evidence of surface passivation, in spite of larger open-circuit voltage. This is likely due to a nonfavorable orientation of the 2D perovskite with respect to methylammonium lead iodide and to the formation of 2D phases with very low dimensionality (pure 2D).

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b02224

Chinese Library Classification Number:

Citation Information:

Low-dimensional (quasi-) 2D perovskites are being extensively studied in order to enhance the stability and the open-circuit voltage of perovskite solar cells. Up to now, thin 2D perovskite layers on the surface and/or at the grain boundaries of 3D perovskites have been deposited solely by solution processing, leading to unavoidable intermixing between the two phases. In this work, we report the fabrication of 2D/3D/2D perovskite heterostructures by dual-source vacuum deposition, with the aim of studying the interaction between the 3D and 2D phases as well as the charge transport properties of 2D perovskites in neat 2D/3D interfaces. Unlike what is normally observed in solution-processed 3D/2D systems, we found a reduced charge transport with no direct evidence of surface passivation, in spite of larger open-circuit voltage. This is likely due to a nonfavorable orientation of the 2D perovskite with respect to methylammonium lead iodide and to the formation of 2D phases with very low dimensionality (pure 2D).

quote

GB/T 7714-2015 [1] MariaGrazia LaPlaca, Lidón GilEscrig, Dengyang Guo, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b02224.
MLA [1] MariaGrazia LaPlaca, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b02224.
APA [1] MariaGrazia LaPlaca, Lidón GilEscrig, Dengyang Guo, Francisco Palazon, Tom J. Savenije, Michele Sessolo, & Henk J. Bolink. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b02224
IEEE [1] MariaGrazia LaPlaca, Lidón GilEscrig, Dengyang Guo, Francisco Palazon, Tom J. Savenije, Michele Sessolo, and Henk J. Bolink, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b02224.