Experimental Discovery of a Fast and Stable Lithium Thioborate Solid Electrolyte, Li6+2x[B10S18]Sx (x ≈ 1) AITranslate

Xiamen University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

High-performance, practical all-solid-state batteries (ASSBs) require solid-state electrolytes (SSEs) with fast Li-ion conduction, wide electrochemical stability window, low cost, and low mass density. Recent density functional theory (DFT) simulations have suggested that lithium thioborates are a particularly promising class of materials for high-performance SSEs in Li batteries, but these materials have not been studied extensively experimentally due to synthesis difficulty. Particularly, their electrochemical properties remain largely underexplored, limiting their further development and application as SSEs. In this work, we report the successful synthesis and a comprehensive electrochemical performance study of single-phase, crystalline Li6+2x[B10S18]Sx (x ≈ 1). We find cold-pressed samples of Li6+2x[B10S18]Sx (x ≈ 1) to exhibit a high ionic conductivity of 1.3 × 10–4 S cm–1 at room temperature. Furthermore, Li6+2x[B10S18]Sx (x ≈ 1) shows an electrochemical stability window of 1.3–2.5 V, much wider than most sulfide SSEs. Symmetrical Li–Li cells fabricated with a Li6+2x[B10S18]Sx (x ≈ 1) pellet were cycled up to a current density of 1 mA cm–2 and exhibited good long-term cycling stability for more than 140 h at 0.3 mA cm–2. These results suggest Li6+2x[B10S18]Sx (x ≈ 1) as a promising choice of SSE for high-performance ASSBs for energy storage.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00560

Chinese Library Classification Number:

Citation Information:

High-performance, practical all-solid-state batteries (ASSBs) require solid-state electrolytes (SSEs) with fast Li-ion conduction, wide electrochemical stability window, low cost, and low mass density. Recent density functional theory (DFT) simulations have suggested that lithium thioborates are a particularly promising class of materials for high-performance SSEs in Li batteries, but these materials have not been studied extensively experimentally due to synthesis difficulty. Particularly, their electrochemical properties remain largely underexplored, limiting their further development and application as SSEs. In this work, we report the successful synthesis and a comprehensive electrochemical performance study of single-phase, crystalline Li6+2x[B10S18]Sx (x ≈ 1). We find cold-pressed samples of Li6+2x[B10S18]Sx (x ≈ 1) to exhibit a high ionic conductivity of 1.3 × 10–4 S cm–1 at room temperature. Furthermore, Li6+2x[B10S18]Sx (x ≈ 1) shows an electrochemical stability window of 1.3–2.5 V, much wider than most sulfide SSEs. Symmetrical Li–Li cells fabricated with a Li6+2x[B10S18]Sx (x ≈ 1) pellet were cycled up to a current density of 1 mA cm–2 and exhibited good long-term cycling stability for more than 140 h at 0.3 mA cm–2. These results suggest Li6+2x[B10S18]Sx (x ≈ 1) as a promising choice of SSE for high-performance ASSBs for energy storage.

quote

GB/T 7714-2015 [1] Yinxing Ma, Jiayu Wan, Xin Xu, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00560.
MLA [1] Yinxing Ma, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00560.
APA [1] Yinxing Ma, Jiayu Wan, Xin Xu, Austin D. Sendek, Sarah E. Holmes, Brandi Ransom, Zhelong Jiang, Pu Zhang, Xin Xiao, Wenbo Zhang, Rong Xu, Fang Liu, Yusheng Ye, Emma Kaeli, Evan J. Reed, William C. Chueh, & Yi Cui. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00560
IEEE [1] Yinxing Ma, Jiayu Wan, Xin Xu, Austin D. Sendek, Sarah E. Holmes, Brandi Ransom, Zhelong Jiang, Pu Zhang, Xin Xiao, Wenbo Zhang, Rong Xu, Fang Liu, Yusheng Ye, Emma Kaeli, Evan J. Reed, William C. Chueh, and Yi Cui, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00560.