Approaching Full-Scale Passivation in Perovskite Solar Cells via Valent-Variable Carbazole Cations AITranslate

Nanjing Tech University; Nanjing Tech University; Nanjing Tech University; Nanjing Tech University; Nanjing Tech University; Nanjing Tech University; Nanjing Tech University; Shanghai Institute of Applied Physics; Nanjing Tech University; Fudan University; Northwestern Polytechnical University (NPU); Nanjing Tech University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hybrid halide perovskite solar cells (PSCs) have emerged as the next-generation photovoltaic technology. Compared to steady silicon solar cells, PSCs are facilely processable but easily generate defects/traps during the thin-film fabrication from the solution. To passivate these defects, which have been considered as the origin of PSC instability, numerous large-sized organic cations (LSOCs) were applied via post-treatment methods. Unfortunately, along with the passivation on defects, these LSOCs could also react with regular perovskite phases and convert them into layered perovskite phases with poorer optoelectronic performances. Herein, we have designed carbazole ethylammonium iodide (CzEAI), a LSOC salt which exhibits a variation from monovalent to divalent state. Importantly, unlike traditional LSOC passivators in monovalent states mostly consumed by a regular perovskite phase and merely affecting the upper domain in thin films, CzEA in monovalent state could penetrate through the whole domain in perovskite films and then accurately convert into a divalent state at defect sites and thus realize a full-scale passivation in PSCs. Both simulation and experimental results proved that a CzEA passivator could overcome the formation of poor optoelectronic layered perovskite phases. As a result, the CzEA passivated PSC demonstrated an optimized photon-to-electron conversion efficiency (PCE) of 24.14% together with a significantly improved long-term stability over 5000 h.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00410

Chinese Library Classification Number:

Citation Information:

Hybrid halide perovskite solar cells (PSCs) have emerged as the next-generation photovoltaic technology. Compared to steady silicon solar cells, PSCs are facilely processable but easily generate defects/traps during the thin-film fabrication from the solution. To passivate these defects, which have been considered as the origin of PSC instability, numerous large-sized organic cations (LSOCs) were applied via post-treatment methods. Unfortunately, along with the passivation on defects, these LSOCs could also react with regular perovskite phases and convert them into layered perovskite phases with poorer optoelectronic performances. Herein, we have designed carbazole ethylammonium iodide (CzEAI), a LSOC salt which exhibits a variation from monovalent to divalent state. Importantly, unlike traditional LSOC passivators in monovalent states mostly consumed by a regular perovskite phase and merely affecting the upper domain in thin films, CzEA in monovalent state could penetrate through the whole domain in perovskite films and then accurately convert into a divalent state at defect sites and thus realize a full-scale passivation in PSCs. Both simulation and experimental results proved that a CzEA passivator could overcome the formation of poor optoelectronic layered perovskite phases. As a result, the CzEA passivated PSC demonstrated an optimized photon-to-electron conversion efficiency (PCE) of 24.14% together with a significantly improved long-term stability over 5000 h.

quote

GB/T 7714-2015 [1] Jingjin Dong, Suhao Yan, Haoyu Chen, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00410.
MLA [1] Jingjin Dong, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00410.
APA [1] Jingjin Dong, Suhao Yan, Haoyu Chen, Ying Chu, Zihao Li, Jinzheng Zhao, Pinghui Yang, Liwei Cheng, Aifei Wang, Yingguo Yang, Wei Huang, & Tianshi Qin. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00410
IEEE [1] Jingjin Dong, Suhao Yan, Haoyu Chen, Ying Chu, Zihao Li, Jinzheng Zhao, Pinghui Yang, Liwei Cheng, Aifei Wang, Yingguo Yang, Wei Huang, and Tianshi Qin, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00410.