daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Critical analysis of laboratory measurements and monitoring system of water-pipe network corrosion-case study. AITranslate

Gdansk University of Technology; Gdansk University of Technology; Gdansk University of Technology; Gdansk University of Technology; Gdansk University of Technology;MPWIK S.A.(Municipal Waterworks in Cracow), Senatorska 1;AGH University of Science and Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Case study of corrosion failure of urban water supply system caused by environmental factors was presented. Nowadays corrosion monitoring of water distribution systems is an object of major concern. There is possibility of application broad range of techniques like gravimetric and electrochemical. Both kinds of techniques can be applied in laboratory and field conditions. In many cases researches limit the case analysis to measurements in laboratory conditions. Presented work contain critical analysis of results obtained in laboratory and field conditions based on corrosion monitoring of three pipelines systems failure in Krakow.

KeyWords AITranslate

Monitoring Corrosion Pipelines EIS Acid rain
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2016.01.004

Chinese Library Classification Number:

Citation Information:

Case study of corrosion failure of urban water supply system caused by environmental factors was presented. Nowadays corrosion monitoring of water distribution systems is an object of major concern. There is possibility of application broad range of techniques like gravimetric and electrochemical. Both kinds of techniques can be applied in laboratory and field conditions. In many cases researches limit the case analysis to measurements in laboratory conditions. Presented work contain critical analysis of results obtained in laboratory and field conditions based on corrosion monitoring of three pipelines systems failure in Krakow.

quote

GB/T 7714-2015 [1] Agata Jazdzewska, Kazimierz Darowicki, Juliusz Orlikowski, et al. Case Studies in Construction Materials, 2016(4). DOI:10.1016/j.cscm.2016.01.004.
MLA [1] Agata Jazdzewska, et al., Case Studies in Construction Materials, no. 4, 2016, https://doi.org/10.1016/j.cscm.2016.01.004.
APA [1] Agata Jazdzewska, Kazimierz Darowicki, Juliusz Orlikowski, Stefan Krakowiak, Krzysztof Zakowski, Maciej Gruszka, & Jacek Banas. (2016). Case Studies in Construction Materials(4). https://doi.org/10.1016/j.cscm.2016.01.004
IEEE [1] Agata Jazdzewska, Kazimierz Darowicki, Juliusz Orlikowski, Stefan Krakowiak, Krzysztof Zakowski, Maciej Gruszka, and Jacek Banas, Case Studies in Construction Materials, no. 4, 2016, doi: 10.1016/j.cscm.2016.01.004. keywords: {Monitoring;Corrosion;Pipelines;EIS;Acid rain}