Towards Commercialization of Graphite as an Anode for Na-ion Batteries: Evolution, Virtues, and Snags of Solvent Cointercalation AITranslate
Abstract AITranslate
Sodium-ion storage in graphite through a solvent cointercalation mechanism is extremely robust regarding cycling stability, rate performance, and Coulombic efficiency. The graphite half cell has a low working voltage and high power density. The respectable capacity, even at high current rates, makes graphite in a glyme-based system a versatile energy storage device. This perspective comprehensively looks at graphite-based sodium-ion full cells and how they perform. Electrolyte composition, cathode working voltage, irreversibility, precycling, and high current performance are the key points to consider during full-cell fabrication. Some general factors to consider during the full-cell assembly are put forward in this perspective.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02295
Chinese Library Classification Number:
Citation Information:
Sodium-ion storage in graphite through a solvent cointercalation mechanism is extremely robust regarding cycling stability, rate performance, and Coulombic efficiency. The graphite half cell has a low working voltage and high power density. The respectable capacity, even at high current rates, makes graphite in a glyme-based system a versatile energy storage device. This perspective comprehensively looks at graphite-based sodium-ion full cells and how they perform. Electrolyte composition, cathode working voltage, irreversibility, precycling, and high current performance are the key points to consider during full-cell fabrication. Some general factors to consider during the full-cell assembly are put forward in this perspective.
quote
| GB/T 7714-2015 | [1] Krishnan Subramanyan, Vanchiappan Aravindan. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02295. |
| MLA | [1] Krishnan Subramanyan, and Vanchiappan Aravindan. ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02295. |
| APA | [1] Krishnan Subramanyan, & Vanchiappan Aravindan. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02295 |
| IEEE | [1] Krishnan Subramanyan and Vanchiappan Aravindan, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02295. |