Recent Progress in Stimulus-Responsive Two-Dimensional Metal–Organic Frameworks AITranslate
Abstract AITranslate
Two-dimensional (2D) metal–organic frameworks (MOFs) play an essential role in response to external stimuli by changing their physical or chemical properties. This Review mainly aims at the recent progress of stimuli-response in 2D MOFs. The various external stimuli, such as ions, solvents, gas, light, electron, temperature, and others, to 2D MOFs are systematically introduced and summarized. In addition, future perspectives relate to 2D MOFs for the stimuli-response are also discussed. We hope that this Review could provide a guideline to help researchers to design new stimuli-response 2D MOFs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.0c00148
Chinese Library Classification Number:
Citation Information:
Two-dimensional (2D) metal–organic frameworks (MOFs) play an essential role in response to external stimuli by changing their physical or chemical properties. This Review mainly aims at the recent progress of stimuli-response in 2D MOFs. The various external stimuli, such as ions, solvents, gas, light, electron, temperature, and others, to 2D MOFs are systematically introduced and summarized. In addition, future perspectives relate to 2D MOFs for the stimuli-response are also discussed. We hope that this Review could provide a guideline to help researchers to design new stimuli-response 2D MOFs.
quote
| GB/T 7714-2015 | [1] Chao Li, Kuaibing Wang, Jingze Li, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00148. |
| MLA | [1] Chao Li, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00148. |
| APA | [1] Chao Li, Kuaibing Wang, Jingze Li, & Qichun Zhang. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00148 |
| IEEE | [1] Chao Li, Kuaibing Wang, Jingze Li, and Qichun Zhang, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00148. |