Manganese MOF Enables Efficient Oxygen Evolution in Acid AITranslate

University of Toronto; University of Toronto; University of Toronto; University of Toronto; University of Toronto; University of Toronto
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The oxygen evolution capabilities of a manganese metal–organic framework (MOF) are demonstrated in acid (pH 1.3) for the first time. The MOF/carbon black composite significantly outperforms MnO2, a known non-noble acidic OER catalyst, exhibiting overpotentials of 539 and 764 mV (vs 715 and 898 mV for MnO2) for a current density of 10 and 50 mA/cm2, respectively.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00123

Chinese Library Classification Number:

Citation Information:

The oxygen evolution capabilities of a manganese metal–organic framework (MOF) are demonstrated in acid (pH 1.3) for the first time. The MOF/carbon black composite significantly outperforms MnO2, a known non-noble acidic OER catalyst, exhibiting overpotentials of 539 and 764 mV (vs 715 and 898 mV for MnO2) for a current density of 10 and 50 mA/cm2, respectively.

quote

GB/T 7714-2015 [1] Kamalpreet Singh, Jose de Jesus Guillen Campos, Filip Dinic, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00123.
MLA [1] Kamalpreet Singh, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00123.
APA [1] Kamalpreet Singh, Jose de Jesus Guillen Campos, Filip Dinic, Zhaomin Hao, Tiange Yuan, & Oleksandr Voznyy. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00123
IEEE [1] Kamalpreet Singh, Jose de Jesus Guillen Campos, Filip Dinic, Zhaomin Hao, Tiange Yuan, and Oleksandr Voznyy, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00123.