daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Design and Synthesis of Shape Memory Phenol-Formaldehyde with Good Irradiation Resistance, Thermal, and Mechanical Properties AITranslate

Harbin Institute of Technology (HIT); Harbin Institute of Technology (HIT); Harbin Institute of Technology (HIT); Harbin Institute of Technology (HIT)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Phenol-formaldehyde (PF) resins with low flammability and excellent ablative property have been widely used in thermal protection systems in the aerospace field. The developing deployable thermal protection structure has prompted further exploration of the possibility of PF resin as a smart polymer. This paper prepares the shape memory phenol-formaldehyde resins (SMPFs) by introducing polyurethane (PU) prepolymer into the resol resin. The SMPFs with crystallization microregion possess excellent shape memory performance and better toughness than PF resin. In addition, the SMPFs have a higher carbon residue rate and better thermal stability compared with other shape memory polymers commonly used in the aerospace field. Multiple test results before and after γ-ray irradiation indicate that SMPFs have excellent irradiation resistance. The oxyacetylene ablative test demonstrates that SMPFs have relatively good ablative resistance. SMPFs inspire the production of intelligent thermal protection systems.

KeyWords AITranslate

shape memory phenolformaldehyde irradiation resistance ablative resistance thermal property
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00719

Chinese Library Classification Number:

Citation Information:

Phenol-formaldehyde (PF) resins with low flammability and excellent ablative property have been widely used in thermal protection systems in the aerospace field. The developing deployable thermal protection structure has prompted further exploration of the possibility of PF resin as a smart polymer. This paper prepares the shape memory phenol-formaldehyde resins (SMPFs) by introducing polyurethane (PU) prepolymer into the resol resin. The SMPFs with crystallization microregion possess excellent shape memory performance and better toughness than PF resin. In addition, the SMPFs have a higher carbon residue rate and better thermal stability compared with other shape memory polymers commonly used in the aerospace field. Multiple test results before and after γ-ray irradiation indicate that SMPFs have excellent irradiation resistance. The oxyacetylene ablative test demonstrates that SMPFs have relatively good ablative resistance. SMPFs inspire the production of intelligent thermal protection systems.

quote

GB/T 7714-2015 [1] Yongdie Deng, Fenghua Zhang, Yanju Liu, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00719.
MLA [1] Yongdie Deng, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00719.
APA [1] Yongdie Deng, Fenghua Zhang, Yanju Liu, & Jinsong Leng. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00719
IEEE [1] Yongdie Deng, Fenghua Zhang, Yanju Liu, and Jinsong Leng, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00719. keywords: {shape memory;phenolformaldehyde;irradiation resistance;ablative resistance;thermal property}