Algal Biomass-Loaded Hydrogel Scaffolds as a Biomimetic Platform with Antibacterial and Wound Healing Activities AITranslate
Abstract AITranslate
The confluence of hydrogel scaffolds and dried algal biomass (AB), consisting of all the bioactive compounds, offers the possibility to facilitate wound healing while simultaneously instilling antibacterial benefits. For this purpose, a single-step synthesis of algal (Chlorella sorokiniana) biomass-loaded hydrogel scaffolds (AHS) was achieved. C. sorokiniana has been used in different areas for several years and has proved attractive to the pharmaceutical and cosmetic industries. Of note, the presence of phytochemicals and various bioactive compounds provides an added health benefit. Hitherto, we report AHS with accelerated wound healing along with potent anti-inflammatory and antibacterial properties. AHS consisting of different concentrations of AB was applied for 14 days on excisional wounds in mice. Microscopic analyses, assessment of proinflammatory and anti-inflammatory cytokines, and histological studies were performed to investigate wound healing. These scaffolds were extensively characterized and studied using Fourier transform infrared, X-ray diffraction, Raman, atomic force microscopy, transmission electron microscopy, scanning electron microscopy, swelling, rheological, thermal, and mechanical analyses. AHS have excellent biocompatibility in addition to significant antibacterial activity against Escherichia coli (99%) and Staphylococcus aureus (98%). We believe that the as-synthesized AHS have the potential to broaden the arsenal of more effective wound healing processes along with antibacterial activities.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00722
Chinese Library Classification Number:
Citation Information:
The confluence of hydrogel scaffolds and dried algal biomass (AB), consisting of all the bioactive compounds, offers the possibility to facilitate wound healing while simultaneously instilling antibacterial benefits. For this purpose, a single-step synthesis of algal (Chlorella sorokiniana) biomass-loaded hydrogel scaffolds (AHS) was achieved. C. sorokiniana has been used in different areas for several years and has proved attractive to the pharmaceutical and cosmetic industries. Of note, the presence of phytochemicals and various bioactive compounds provides an added health benefit. Hitherto, we report AHS with accelerated wound healing along with potent anti-inflammatory and antibacterial properties. AHS consisting of different concentrations of AB was applied for 14 days on excisional wounds in mice. Microscopic analyses, assessment of proinflammatory and anti-inflammatory cytokines, and histological studies were performed to investigate wound healing. These scaffolds were extensively characterized and studied using Fourier transform infrared, X-ray diffraction, Raman, atomic force microscopy, transmission electron microscopy, scanning electron microscopy, swelling, rheological, thermal, and mechanical analyses. AHS have excellent biocompatibility in addition to significant antibacterial activity against Escherichia coli (99%) and Staphylococcus aureus (98%). We believe that the as-synthesized AHS have the potential to broaden the arsenal of more effective wound healing processes along with antibacterial activities.
quote
| GB/T 7714-2015 | [1] Aakanksha Agarwal, Arun Kumar, Piyush Garg, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00722. |
| MLA | [1] Aakanksha Agarwal, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00722. |
| APA | [1] Aakanksha Agarwal, Arun Kumar, Piyush Garg, Arnab Chakraborty, Ranjan Verma, Maryam Sarwat, Ajay Gupta, Pijus K. Sasmal, Yogesh Kumar Verma, Chiranjit Chowdhury, & Monalisa Mukherjee. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00722 |
| IEEE | [1] Aakanksha Agarwal, Arun Kumar, Piyush Garg, Arnab Chakraborty, Ranjan Verma, Maryam Sarwat, Ajay Gupta, Pijus K. Sasmal, Yogesh Kumar Verma, Chiranjit Chowdhury, and Monalisa Mukherjee, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00722. keywords: {microalgae;biomass;hydrogel scaffold;wound healing;antibacterial activity} |