daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Opportunities of Ionomer Development for Anion-Exchange Membrane Water Electrolysis AITranslate

Energy, Mining & Environment Research Centre; 8888 University Drive; 8888 University Drive
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Anion-exchange membrane water electrolysis (AEM-WE) promises low cost, green hydrogen production for the future. In order to meet this potential, significant improvements to the performance and stability of catalyst layers (CLs) must be made, including the development of tailor-made ion conducting polymer materials. This Focus Review outlines the role of anion-exchange ionomers (AEIs) in CLs for enabling catalyst activation, enhancing stability toward delamination, and improving ion conduction. Detrimental effects such as inhibition of the hydrogen evolution reaction (HER) and oxygen evolution reaction (OER) and oxidative instability of the ionomer are also discussed with key findings from recent AEM-WE literature. Opportunities for future ionomer development are discussed to guide such efforts.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01040

Chinese Library Classification Number:

Citation Information:

Anion-exchange membrane water electrolysis (AEM-WE) promises low cost, green hydrogen production for the future. In order to meet this potential, significant improvements to the performance and stability of catalyst layers (CLs) must be made, including the development of tailor-made ion conducting polymer materials. This Focus Review outlines the role of anion-exchange ionomers (AEIs) in CLs for enabling catalyst activation, enhancing stability toward delamination, and improving ion conduction. Detrimental effects such as inhibition of the hydrogen evolution reaction (HER) and oxygen evolution reaction (OER) and oxidative instability of the ionomer are also discussed with key findings from recent AEM-WE literature. Opportunities for future ionomer development are discussed to guide such efforts.

quote

GB/T 7714-2015 [1] Peter Mardle, Binyu Chen, Steven Holdcroft. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01040.
MLA [1] Peter Mardle, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01040.
APA [1] Peter Mardle, Binyu Chen, & Steven Holdcroft. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01040
IEEE [1] Peter Mardle, Binyu Chen, and Steven Holdcroft, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01040.