daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Pathways to High-Power-Density Redox Flow Batteries AITranslate

Harvard University; Technion−Israel Institute of Technology; Technion−Israel Institute of Technology; Harvard University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Redox flow batteries (RFBs) promise to fill a crucial missing link in the energy transition: inexpensive and widely deployable grid and industrial-scale energy storage for intermittent renewable electricity. While numerous lab-scale and demonstration-scale RFBs have been delivered, widespread commercial deployment is still limited by high electrolyte, stack, and balance of plant capital costs. Increasing the power density of RFBs is correlated with lower stack costs, primarily because the area needed for expensive electrode and membrane components to reach a target power density is reduced. In the present contribution, we summarize the areal power densities reported for lab-scale RFBs, critically evaluate major pathways employed for power optimization, and identify opportunities for developing yet-higher power density systems.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01043

Chinese Library Classification Number:

Citation Information:

Redox flow batteries (RFBs) promise to fill a crucial missing link in the energy transition: inexpensive and widely deployable grid and industrial-scale energy storage for intermittent renewable electricity. While numerous lab-scale and demonstration-scale RFBs have been delivered, widespread commercial deployment is still limited by high electrolyte, stack, and balance of plant capital costs. Increasing the power density of RFBs is correlated with lower stack costs, primarily because the area needed for expensive electrode and membrane components to reach a target power density is reduced. In the present contribution, we summarize the areal power densities reported for lab-scale RFBs, critically evaluate major pathways employed for power optimization, and identify opportunities for developing yet-higher power density systems.

quote

GB/T 7714-2015 [1] Kiana Amini, Amit N. Shocron, Matthew E. Suss, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01043.
MLA [1] Kiana Amini, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01043.
APA [1] Kiana Amini, Amit N. Shocron, Matthew E. Suss, & Michael J. Aziz. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01043
IEEE [1] Kiana Amini, Amit N. Shocron, Matthew E. Suss, and Michael J. Aziz, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01043.