Eco-efficiency evaluation of sustainable self-compacting concrete using magnesite mine waste AITranslate

Vellore Institute of Technology;Vellore Institute of Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Utilization potential of industrial by-products/wastes as construction material requires adequate workability, strength and other required properties as specified by standard codes of practice and certain sustainability criteria. Coal combustion byproduct (fly ash) and mine waste are a few of the abundantly available wastes that create a challenging task in their disposal with the current practice of dumping on-sites and landfilling. This study enumerates the suitability of utilizing magnesite mine wastes in self-compacting concrete (SCC) as binder and aggregate replacements by considering the evaluation factors such as fresh, hardened properties, life cycle assessment (LCA) and eco-efficiency. The results from the experimental investigation revealed that aggregate blended SCC performed well in terms of both fresh and mechanical properties, while cement blended mixtures exhibited satisfactory results. Additionally, fly ash and magnesite mine waste substantially reduced CO2 emissions and costs with added strength benefits. Eco-efficiency evaluation of mine waste blended SCC reported up to 75% higher efficiency than conventional SCC.

KeyWords AITranslate

Sustainable SCC Mine waste CO2 emission Cost analysis Ecostrength efficiency
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2023.e02765

Chinese Library Classification Number:

Citation Information:

Utilization potential of industrial by-products/wastes as construction material requires adequate workability, strength and other required properties as specified by standard codes of practice and certain sustainability criteria. Coal combustion byproduct (fly ash) and mine waste are a few of the abundantly available wastes that create a challenging task in their disposal with the current practice of dumping on-sites and landfilling. This study enumerates the suitability of utilizing magnesite mine wastes in self-compacting concrete (SCC) as binder and aggregate replacements by considering the evaluation factors such as fresh, hardened properties, life cycle assessment (LCA) and eco-efficiency. The results from the experimental investigation revealed that aggregate blended SCC performed well in terms of both fresh and mechanical properties, while cement blended mixtures exhibited satisfactory results. Additionally, fly ash and magnesite mine waste substantially reduced CO2 emissions and costs with added strength benefits. Eco-efficiency evaluation of mine waste blended SCC reported up to 75% higher efficiency than conventional SCC.

quote

GB/T 7714-2015 [1] Pitchiah Raman Shunmuga Vembu, Arun Kumar Ammasi. Case Studies in Construction Materials, 2024(20). DOI:10.1016/j.cscm.2023.e02765.
MLA [1] Pitchiah Raman Shunmuga Vembu, and Arun Kumar Ammasi. Case Studies in Construction Materials, no. 20, 2024, https://doi.org/10.1016/j.cscm.2023.e02765.