Additive manufacturing of digitally programmable hierarchical biomimetic surfaces for hydrodynamic informatics AITranslate

Kookmin University; Kumoh National Institute of Technology; Kookmin University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Herein, combinatorial biomimetic hierarchical micro/nanoscale structures (HMNSs) inspired by lotus leaves and rose petals are realized on a single copper (Cu) substrate via laser-induced reductive clustering (LRC) of copper(II) oxide nanoparticles. Cu spike structures are constructed via mild LRC to imitate microscale papillae of the lotus leaf surface. Subsequently, the LRC-treated specimen is immersed in a 1H,1H,2H,2H‐perfluorooctyltrichlorosilane (PFOTS) solution for emulating the high-density nanopillars on the conical microcells of the lotus leaf. The microscale surface texture for achieving the rose-petal effect is realized by forming a microporous Cu-chain structure via intense LRC based on prolonged laser heating. By soaking the microporous Cu-chain structure in a PFOTS solution, the rose petal–inspired HMNS is demonstrated. The created lotus leaf– and rose petal–inspired HMNSs exhibit water rolling and droplet-pinning wetting characteristics, respectively. These HMNSs are selectively patterned and customized in a digitally programmable manner on a single Cu plate for fabricating a hydrodynamic memory device that can save and display digital data. Owing to its additive manufacturing feature, the developed LRC method could be applied to a wide spectrum of substrates ranging from glass to flexible plastics.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2023.103763

Chinese Library Classification Number:

Citation Information:

Herein, combinatorial biomimetic hierarchical micro/nanoscale structures (HMNSs) inspired by lotus leaves and rose petals are realized on a single copper (Cu) substrate via laser-induced reductive clustering (LRC) of copper(II) oxide nanoparticles. Cu spike structures are constructed via mild LRC to imitate microscale papillae of the lotus leaf surface. Subsequently, the LRC-treated specimen is immersed in a 1H,1H,2H,2H‐perfluorooctyltrichlorosilane (PFOTS) solution for emulating the high-density nanopillars on the conical microcells of the lotus leaf. The microscale surface texture for achieving the rose-petal effect is realized by forming a microporous Cu-chain structure via intense LRC based on prolonged laser heating. By soaking the microporous Cu-chain structure in a PFOTS solution, the rose petal–inspired HMNS is demonstrated. The created lotus leaf– and rose petal–inspired HMNSs exhibit water rolling and droplet-pinning wetting characteristics, respectively. These HMNSs are selectively patterned and customized in a digitally programmable manner on a single Cu plate for fabricating a hydrodynamic memory device that can save and display digital data. Owing to its additive manufacturing feature, the developed LRC method could be applied to a wide spectrum of substrates ranging from glass to flexible plastics.

quote

GB/T 7714-2015 [1] Jibi Jais, Jung Hwan Park, Bongchul Kang. Additive Manufacturing, 2023(76). DOI:10.1016/j.addma.2023.103763.
MLA [1] Jibi Jais, et al., Additive Manufacturing, no. 76, 2023, https://doi.org/10.1016/j.addma.2023.103763.
APA [1] Jibi Jais, Jung Hwan Park, & Bongchul Kang. (2023). Additive Manufacturing(76). https://doi.org/10.1016/j.addma.2023.103763
IEEE [1] Jibi Jais, Jung Hwan Park, and Bongchul Kang, Additive Manufacturing, no. 76, 2023, doi: 10.1016/j.addma.2023.103763.