This study investigated the process of fabricating a bimetallic structure of 316L stainless steel (SS) and 4043 aluminum (Al) using wire-arc directed energy deposition (DED) based on the cold metal transfer (CMT) process. The impact of heat input on the fabricated structure’s geometry, porosity, and microstructures at the interface, with a specific emphasis on the intermetallic compound (IMC) formation, and the subsequent impact on the joint strength of the structure, were studied. The IMC layer at the interface was predominantly comprised of FeAl2Si. For the various heat input conditions studied, the IMC layer`s thickness varied from 5 µm to 18 µm. The tensile strength reached up to approximately 130 MPa, which is among the highest reported in the literature for steel/Al bimetallic structures. The specimens fabricated with high heat input conditions had a thicker IMC layer at the steel/Al interface, resulting in a more brittle interface and degradation of the mechanical properties.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.addma.2024.104015
Chinese Library Classification Number:
Citation Information:
This study investigated the process of fabricating a bimetallic structure of 316L stainless steel (SS) and 4043 aluminum (Al) using wire-arc directed energy deposition (DED) based on the cold metal transfer (CMT) process. The impact of heat input on the fabricated structure’s geometry, porosity, and microstructures at the interface, with a specific emphasis on the intermetallic compound (IMC) formation, and the subsequent impact on the joint strength of the structure, were studied. The IMC layer at the interface was predominantly comprised of FeAl2Si. For the various heat input conditions studied, the IMC layer`s thickness varied from 5 µm to 18 µm. The tensile strength reached up to approximately 130 MPa, which is among the highest reported in the literature for steel/Al bimetallic structures. The specimens fabricated with high heat input conditions had a thicker IMC layer at the steel/Al interface, resulting in a more brittle interface and degradation of the mechanical properties.
quote
| GB/T 7714-2015 | [1] Md Abdul Karim, Sainand Jadhav, Rangasayee Kannan, et al. Additive Manufacturing, 2024(81). DOI:10.1016/j.addma.2024.104015. |
| MLA | [1] Md Abdul Karim, et al., Additive Manufacturing, no. 81, 2024, https://doi.org/10.1016/j.addma.2024.104015. |
| APA | [1] Md Abdul Karim, Sainand Jadhav, Rangasayee Kannan, Dean Pierce, Yousub Lee, Peeyush Nandwana, & Duck Bong Kim. (2024). Additive Manufacturing(81). https://doi.org/10.1016/j.addma.2024.104015 |
| IEEE | [1] Md Abdul Karim, Sainand Jadhav, Rangasayee Kannan, Dean Pierce, Yousub Lee, Peeyush Nandwana, and Duck Bong Kim, Additive Manufacturing, no. 81, 2024, doi: 10.1016/j.addma.2024.104015. |