Click Chemistry for Linker-Free BAMO-Based Energetic Sequence-Controlled Copolymers AITranslate

Nanjing University of Science and Technology; Nanjing University of Science and Technology;Shanghai Space Propulsion Technology Research Institute; Nanjing University of Science and Technology; Nanjing University of Science and Technology; Nanjing University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In the field of energetic materials (EMs), soft chains are copolymerized with energetic polymers to improve flexibility. However, this often makes it difficult to achieve simultaneous optimization of the energy level and flexibility due to the random sequence. In this study, a simple approach is presented to develop energetic sequence-controlled polymers (ESCPs), alternate copolymers poly(3,3-bis(azidomethyl)oxetane-glycol) (P(BAMO-alt-EG)) and poly(3,3-bis(azidomethyl)oxetane-tetrahydrofuran) (P(BAMO-alt-THF)), through click reactions. This approach provides the potential to design and control mechanical and thermal properties in propellant binders by introducing various segments and regulating the sequence structure. These polymers display excellent thermal stability and demonstrate that regulated shorter segmental length promoted better flexibility and less residual carbon content without compromising the energy level of the propellant. The obtained kinetic parameters prove that P(BAMO-alt-EG) released higher heat and accelerated the thermolysis process compared to P(BAMO-alt-THF). These results demonstrate the potential of highly alternating ESCPs as a potential energetic propellant binder.

KeyWords AITranslate

click chemistry energetic sequencecontrolled polymers glass transition temperature molecular dynamics propellants
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01951

Chinese Library Classification Number:

Citation Information:

In the field of energetic materials (EMs), soft chains are copolymerized with energetic polymers to improve flexibility. However, this often makes it difficult to achieve simultaneous optimization of the energy level and flexibility due to the random sequence. In this study, a simple approach is presented to develop energetic sequence-controlled polymers (ESCPs), alternate copolymers poly(3,3-bis(azidomethyl)oxetane-glycol) (P(BAMO-alt-EG)) and poly(3,3-bis(azidomethyl)oxetane-tetrahydrofuran) (P(BAMO-alt-THF)), through click reactions. This approach provides the potential to design and control mechanical and thermal properties in propellant binders by introducing various segments and regulating the sequence structure. These polymers display excellent thermal stability and demonstrate that regulated shorter segmental length promoted better flexibility and less residual carbon content without compromising the energy level of the propellant. The obtained kinetic parameters prove that P(BAMO-alt-EG) released higher heat and accelerated the thermolysis process compared to P(BAMO-alt-THF). These results demonstrate the potential of highly alternating ESCPs as a potential energetic propellant binder.

quote

GB/T 7714-2015 [1] Yanan Li, Wenfang Zheng, Shengjie Yin, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c01951.
MLA [1] Yanan Li, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c01951.
APA [1] Yanan Li, Wenfang Zheng, Shengjie Yin, Renming Pan, Wenxi Li, & Xiangyang Lin. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c01951
IEEE [1] Yanan Li, Wenfang Zheng, Shengjie Yin, Renming Pan, Wenxi Li, and Xiangyang Lin, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c01951. keywords: {click chemistry;energetic sequencecontrolled polymers;glass transition temperature;molecular dynamics;propellants}