Interfacial Structure Analyses of Single Carbon Fiber-Embedded Polymers by In Situ X-ray Scattering and Birefringence Measurements AITranslate

Kyushu University; Kyushu University; Kyushu University; Kyushu University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Single carbon fiber (CF)-embedded thermoset epoxy resin (EP) and thermoplastic polycarbonate (PC) specimens were prepared to clarify the interfacial interaction between CF and a matrix polymer and the deformation behavior of the carbon fiber and a matrix polymer. Stress–strain curves of EP and PC samples including and excluding CFs showed yields at approximately 70 MPa. In situ polarized high-speed camera images of the samples revealed the effect of CF on stress propagation. Moreover, the retardation of the fiber/polymer interface was large and that of PC was higher than that of EP. Microbeam small/wide-angle X-ray scattering measurements revealed that the orientation of the polymer chains near the CF and the turbostratic structure of the CFs occurred for both EP and PC; craze formation was suppressed because of CF during the deformation process for PC.

KeyWords AITranslate

carbon fiber epoxy resin polycarbonate small/wideangle Xray scattering birefringence interfacial properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01959

Chinese Library Classification Number:

Citation Information:

Single carbon fiber (CF)-embedded thermoset epoxy resin (EP) and thermoplastic polycarbonate (PC) specimens were prepared to clarify the interfacial interaction between CF and a matrix polymer and the deformation behavior of the carbon fiber and a matrix polymer. Stress–strain curves of EP and PC samples including and excluding CFs showed yields at approximately 70 MPa. In situ polarized high-speed camera images of the samples revealed the effect of CF on stress propagation. Moreover, the retardation of the fiber/polymer interface was large and that of PC was higher than that of EP. Microbeam small/wide-angle X-ray scattering measurements revealed that the orientation of the polymer chains near the CF and the turbostratic structure of the CFs occurred for both EP and PC; craze formation was suppressed because of CF during the deformation process for PC.

quote

GB/T 7714-2015 [1] Masatoshi Todaka, Kakeru Obayashi, Ryosuke Kawatoko, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c01959.
MLA [1] Masatoshi Todaka, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c01959.
APA [1] Masatoshi Todaka, Kakeru Obayashi, Ryosuke Kawatoko, & Ken Kojio. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c01959
IEEE [1] Masatoshi Todaka, Kakeru Obayashi, Ryosuke Kawatoko, and Ken Kojio, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c01959. keywords: {carbon fiber;epoxy resin;polycarbonate;small/wideangle Xray scattering;birefringence;interfacial properties}