daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Perovskite Cluster-Containing Solution for Scalable D-Bar Coating toward High-Throughput Perovskite Solar Cells AITranslate

Sungkyunkwan University; Sungkyunkwan University; Sungkyunkwan University; Sogang University; Sungkyunkwan University; Sungkyunkwan University; Sogang University; Sungkyunkwan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

For scalable perovskite solar cells (PSCs), deposition of a homogeneous and high-quality perovskite film on a large area (>100 cm2) is a prerequisite. Conventional solutions for spin-coating on small areas usually contain polar aprotic solvents with high boiling point, which is difficult to adopt for large-area bar coating because of the uncontrollable and slow drying process due to the strong interaction between polar aprotic solvent and Lewis acidic PbI2 or perovskite. Thus, the precursor solution plays a vital role in the success of large-area coating. Here we report a coating solution suitable for large-area perovskite films. The coating solutions prepared via gas-mediated solid–liquid conversion contain preformed perovskite clusters as confirmed by rotational mode of methylammonium cation in the PbI3– framework from Raman spectroscopy. CH3NH3PbI3 (MAPbI3) films formed by D-bar coating within 20 s on the area over 100 cm2 exhibit tetragonal/cubic superlattice structure with highly preferred orientation in the entire film, which results in average power conversion efficiency (PCE) of 17.01% and best PCE of 17.82%.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00042

Chinese Library Classification Number:

Citation Information:

For scalable perovskite solar cells (PSCs), deposition of a homogeneous and high-quality perovskite film on a large area (>100 cm2) is a prerequisite. Conventional solutions for spin-coating on small areas usually contain polar aprotic solvents with high boiling point, which is difficult to adopt for large-area bar coating because of the uncontrollable and slow drying process due to the strong interaction between polar aprotic solvent and Lewis acidic PbI2 or perovskite. Thus, the precursor solution plays a vital role in the success of large-area coating. Here we report a coating solution suitable for large-area perovskite films. The coating solutions prepared via gas-mediated solid–liquid conversion contain preformed perovskite clusters as confirmed by rotational mode of methylammonium cation in the PbI3– framework from Raman spectroscopy. CH3NH3PbI3 (MAPbI3) films formed by D-bar coating within 20 s on the area over 100 cm2 exhibit tetragonal/cubic superlattice structure with highly preferred orientation in the entire film, which results in average power conversion efficiency (PCE) of 17.01% and best PCE of 17.82%.

quote

GB/T 7714-2015 [1] DongNyuk Jeong, DoKyoung Lee, Seongrok Seo, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00042.
MLA [1] DongNyuk Jeong, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00042.
APA [1] DongNyuk Jeong, DoKyoung Lee, Seongrok Seo, Soo Yeon Lim, Yong Zhang, Hyunjung Shin, Hyeonsik Cheong, & NamGyu Park. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00042
IEEE [1] DongNyuk Jeong, DoKyoung Lee, Seongrok Seo, Soo Yeon Lim, Yong Zhang, Hyunjung Shin, Hyeonsik Cheong, and NamGyu Park, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00042.