Defects in Lead Halide Perovskite Nanocrystals: Analogies and (Many) Differences with the Bulk AITranslate

Department of Theoretical Chemistry, Vrije Universiteit Amsterdam;Department of Theoretical Chemistry, Vrije Universiteit Amsterdam;Department of Theoretical Chemistry, Vrije Universiteit Amsterdam
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Understanding the origin of defects in lead halide perovskite nanocrystals is paramount to attaining long-term structural stability and improved optical efficiency, key features for their successful implementation in optoelectronic devices. Unlike other studies, we explore the possible formation of trap states in explicit, nonperiodic CsPbBr3 nanocrystal models about 3 nm in size. Using density functional theory, we compute the defect formation energies of interstitial, vacancy, and antisite defects in different regions of the nanocrystal (center, surface center, and surface edge), demonstrating that the most stable defect position is found at the surface. We ascribe the high defect tolerance of CsPbBr3 nanocrystals to the fact that vacancies, i.e. the loss of surface ligands as ion pairs, are energetically difficult to form and only excessive stripping of surface ligands might be problematic, as their detachment leaves undercoordinated Br– on the crystal surface that only in this case translates into deep traps.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01945

Chinese Library Classification Number:

Citation Information:

Understanding the origin of defects in lead halide perovskite nanocrystals is paramount to attaining long-term structural stability and improved optical efficiency, key features for their successful implementation in optoelectronic devices. Unlike other studies, we explore the possible formation of trap states in explicit, nonperiodic CsPbBr3 nanocrystal models about 3 nm in size. Using density functional theory, we compute the defect formation energies of interstitial, vacancy, and antisite defects in different regions of the nanocrystal (center, surface center, and surface edge), demonstrating that the most stable defect position is found at the surface. We ascribe the high defect tolerance of CsPbBr3 nanocrystals to the fact that vacancies, i.e. the loss of surface ligands as ion pairs, are energetically difficult to form and only excessive stripping of surface ligands might be problematic, as their detachment leaves undercoordinated Br– on the crystal surface that only in this case translates into deep traps.

quote

GB/T 7714-2015 [1] Stephanie ten Brinck, Francesco Zaccaria, Ivan Infante. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01945.
MLA [1] Stephanie ten Brinck, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01945.
APA [1] Stephanie ten Brinck, Francesco Zaccaria, & Ivan Infante. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01945
IEEE [1] Stephanie ten Brinck, Francesco Zaccaria, and Ivan Infante, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01945.