The effect of the source of cement SO3 on the expansion of mortars AITranslate
Abstract AITranslate
In order to evaluate the risk of the source and quantity of cement SO3 on the expansion properties of mortars, this paper studied the influence of Gypsum, Bassanite and clinker sulfate on the cement paste expansion and the formation of delayed ettringite. The investigation covers the mortar cured at 20 °C and 80 °C and stored in water. In contradiction to many studies, the results showed that the cement produced with high sulfur clinker had lower expansion than that produced with classical gypsum or high soluble Bassanite. In addition to that, we have detected that the percentage of SO3, in the cement, could increase the risk of DEF if it surpasses the level of 3.5%. Also, the curing temperature at 80 °C affects the microstructure of concrete by generating cracks in the cement paste.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.cscm.2015.12.004
Chinese Library Classification Number:
Citation Information:
In order to evaluate the risk of the source and quantity of cement SO3 on the expansion properties of mortars, this paper studied the influence of Gypsum, Bassanite and clinker sulfate on the cement paste expansion and the formation of delayed ettringite. The investigation covers the mortar cured at 20 °C and 80 °C and stored in water. In contradiction to many studies, the results showed that the cement produced with high sulfur clinker had lower expansion than that produced with classical gypsum or high soluble Bassanite. In addition to that, we have detected that the percentage of SO3, in the cement, could increase the risk of DEF if it surpasses the level of 3.5%. Also, the curing temperature at 80 °C affects the microstructure of concrete by generating cracks in the cement paste.
quote
| GB/T 7714-2015 | [1] Sayed Horkoss, Gilles Escadeillas, Toufic Rizk, et al. Case Studies in Construction Materials, 2016(4). DOI:10.1016/j.cscm.2015.12.004. |
| MLA | [1] Sayed Horkoss, et al., Case Studies in Construction Materials, no. 4, 2016, https://doi.org/10.1016/j.cscm.2015.12.004. |
| APA | [1] Sayed Horkoss, Gilles Escadeillas, Toufic Rizk, & Roger Lteif. (2016). Case Studies in Construction Materials(4). https://doi.org/10.1016/j.cscm.2015.12.004 |
| IEEE | [1] Sayed Horkoss, Gilles Escadeillas, Toufic Rizk, and Roger Lteif, Case Studies in Construction Materials, no. 4, 2016, doi: 10.1016/j.cscm.2015.12.004. keywords: {Delayed Ettringite Formation;Source of SO3;Expansion;Gypsum;Bassanite;Solubility} |