Tailoring Rigid Segments in Dopant-Free Polymeric Hole Transport Materials for Perovskite Quantum Dot Solar Cells AITranslate

Pohang University of Science and Technology (POSTECH); Pohang University of Science and Technology (POSTECH); Pohang University of Science and Technology (POSTECH); Ajou University; Pohang University of Science and Technology (POSTECH); Pohang University of Science and Technology (POSTECH); Daegu Gyeongbuk Institute of Science and Technology (DGIST); Kookmin University; Ajou University; Pohang University of Science and Technology (POSTECH); Pohang University of Science and Technology (POSTECH)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The dominant hole transport material (HTM) used in perovskite quantum dot solar cells (PQD-SCs) is a Spiro-OMeTAD, which inevitably requires doping systems to increase charge mobility. However, the use of deliquescent dopants leads to the degradation of PQD-SCs, necessitating the development of efficient dopant-free HTMs for their commercialization. Here, we designed three types of dopant-free HTMs: Asy-PDTS, Asy-PSDTS, and Asy-PSeDTS. We apply chalcogenide-based fluorinated benzothiadiazole as a rigid segment acceptor unit to generate an effective charge hopping channel, compensating for the impaired electrical property through side chain engineering. The rigid segment is constructed into favorable planar structures of face-to-face stacking by a conformation-locking approach via chalcogenide–fluorine noncovalent interactions (S···F and Se···F). The optimized device using Asy-PSeDTS achieved 15.2% power conversion efficiency (PCE) and maintained 80% of the initial PCE after 40 days, which is the highest PCE and stability among dopant-free HTM-based PQD-SCs so far.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00211

Chinese Library Classification Number:

Citation Information:

The dominant hole transport material (HTM) used in perovskite quantum dot solar cells (PQD-SCs) is a Spiro-OMeTAD, which inevitably requires doping systems to increase charge mobility. However, the use of deliquescent dopants leads to the degradation of PQD-SCs, necessitating the development of efficient dopant-free HTMs for their commercialization. Here, we designed three types of dopant-free HTMs: Asy-PDTS, Asy-PSDTS, and Asy-PSeDTS. We apply chalcogenide-based fluorinated benzothiadiazole as a rigid segment acceptor unit to generate an effective charge hopping channel, compensating for the impaired electrical property through side chain engineering. The rigid segment is constructed into favorable planar structures of face-to-face stacking by a conformation-locking approach via chalcogenide–fluorine noncovalent interactions (S···F and Se···F). The optimized device using Asy-PSeDTS achieved 15.2% power conversion efficiency (PCE) and maintained 80% of the initial PCE after 40 days, which is the highest PCE and stability among dopant-free HTM-based PQD-SCs so far.

quote

GB/T 7714-2015 [1] Dae Hwan Lee, Seyeong Lim, Chanhyeok Kim, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00211.
MLA [1] Dae Hwan Lee, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00211.
APA [1] Dae Hwan Lee, Seyeong Lim, Chanhyeok Kim, Han Uk Lee, Dasol Chung, Yelim Choi, Jongmin Choi, Younghoon Kim, Sung Beom Cho, Hong Il Kim, & Taiho Park. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00211
IEEE [1] Dae Hwan Lee, Seyeong Lim, Chanhyeok Kim, Han Uk Lee, Dasol Chung, Yelim Choi, Jongmin Choi, Younghoon Kim, Sung Beom Cho, Hong Il Kim, and Taiho Park, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00211.