Buried Guanidinium Passivator with Favorable Binding Energy for Perovskite Solar Cells AITranslate

Chongqing University; Ulsan National Institute of Science and Technology (UNIST); Ulsan National Institute of Science and Technology (UNIST); Ulsan National Institute of Science and Technology (UNIST); Ulsan National Institute of Science and Technology (UNIST); Chongqing University; Chongqing University; Fudan University; Ulsan National Institute of Science and Technology (UNIST); Chongqing University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Rational design and modification of the buried interface toward high performance perovskite solar cells (PSCs) are highly desired and challenging. Here, we demonstrate a series of guanidinium passivators with multiamine substitutions to shed light on the effective passivation geometry at the SnO2/perovskite heterojunction interface. Comparative theoretical and experimental studies reveal that the binding geometry of the highly polarized imine moiety in guanidinium passivators dominates its energetically favorable passivation on the SnO2 surface, which decreases the trap density to 1.11 × 1016 cm–3 with reduced interior/interface nonradiative recombination in the unsymmetrical aminoguanidine hydrochloride (Agu) platform. Consequently, the PSCs with buried Agu passivator deliver a champion power conversion efficiency (PCE) of 24.4% with an advanced open-circuit voltage (VOC) of 1.197 V and prolonged lifetime over 90% of the initial PCE after 900 h in ambient conditions.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02881

Chinese Library Classification Number:

Citation Information:

Rational design and modification of the buried interface toward high performance perovskite solar cells (PSCs) are highly desired and challenging. Here, we demonstrate a series of guanidinium passivators with multiamine substitutions to shed light on the effective passivation geometry at the SnO2/perovskite heterojunction interface. Comparative theoretical and experimental studies reveal that the binding geometry of the highly polarized imine moiety in guanidinium passivators dominates its energetically favorable passivation on the SnO2 surface, which decreases the trap density to 1.11 × 1016 cm–3 with reduced interior/interface nonradiative recombination in the unsymmetrical aminoguanidine hydrochloride (Agu) platform. Consequently, the PSCs with buried Agu passivator deliver a champion power conversion efficiency (PCE) of 24.4% with an advanced open-circuit voltage (VOC) of 1.197 V and prolonged lifetime over 90% of the initial PCE after 900 h in ambient conditions.

quote

GB/T 7714-2015 [1] Bo Zhang, Jiyeon Oh, Zhe Sun, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02881.
MLA [1] Bo Zhang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02881.
APA [1] Bo Zhang, Jiyeon Oh, Zhe Sun, Yongjoon Cho, Seonghun Jeong, Xiao Chen, Kuan Sun, Feng Li, Changduk Yang, & Shanshan Chen. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02881
IEEE [1] Bo Zhang, Jiyeon Oh, Zhe Sun, Yongjoon Cho, Seonghun Jeong, Xiao Chen, Kuan Sun, Feng Li, Changduk Yang, and Shanshan Chen, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02881.