Machine Learning for Understanding Compatibility of Organic–Inorganic Hybrid Perovskites with Post-Treatment Amines AITranslate

The Ohio State University; University of Science and Technology of China; The Ohio State University; The Ohio State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Post-treatment is one of the facile and effective approaches to stabilize organic–inorganic hybrid perovskites. In this work, we apply a machine learning technique to study the trend of reactivity of different types of amines, which are used for the post-treatment of organic–inorganic hybrid perovskite films. Fifty amines are classified based on their compatibility with the methylammonium lead iodide films. Machine learning models are constructed from the classification of these amines and their molecular descriptor features. The model has achieved 86% accuracy on predicting the outcomes of whether perovskite films are maintained after post-treatment. By analyzing the constructed models, it was found that amines with fewer hydrogen bond donors and acceptors, more steric bulk, secondary, tertiary amines, and pyridine derivatives tend to have high compatibility with perovskite films.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b02451

Chinese Library Classification Number:

Citation Information:

Post-treatment is one of the facile and effective approaches to stabilize organic–inorganic hybrid perovskites. In this work, we apply a machine learning technique to study the trend of reactivity of different types of amines, which are used for the post-treatment of organic–inorganic hybrid perovskite films. Fifty amines are classified based on their compatibility with the methylammonium lead iodide films. Machine learning models are constructed from the classification of these amines and their molecular descriptor features. The model has achieved 86% accuracy on predicting the outcomes of whether perovskite films are maintained after post-treatment. By analyzing the constructed models, it was found that amines with fewer hydrogen bond donors and acceptors, more steric bulk, secondary, tertiary amines, and pyridine derivatives tend to have high compatibility with perovskite films.

quote

GB/T 7714-2015 [1] Yongze Yu, Xuanheng Tan, Shougui Ning, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b02451.
MLA [1] Yongze Yu, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b02451.
APA [1] Yongze Yu, Xuanheng Tan, Shougui Ning, & Yiying Wu. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b02451
IEEE [1] Yongze Yu, Xuanheng Tan, Shougui Ning, and Yiying Wu, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b02451.