Partially Dissociated Water Dimers at the Water–Hematite Interface AITranslate

Institute of Applied Physics;Institute of Applied Physics;Institute of Materials Chemistry;Institute of Applied Physics;Institute of Applied Physics;Institute of Applied Physics;Institute of Applied Physics;Institute of Applied Physics;Institute of Applied Physics;Institute of Applied Physics;Institute of Applied Physics;Institute of Materials Chemistry;Institute of Applied Physics
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The oxygen evolution reaction (OER) is thought to occur via a four-step mechanism with *O, *OH, and *OOH as adsorbed intermediates. Linear scaling of the *OH and **OOH adsorption energies is proposed to limit the oxides’ efficiency as OER catalysts, but the use of simple descriptors to screen candidate materials neglects potentially important water–water interactions. Here, we use a combination of temperature-programmed desorption (TPD), X-ray photoemission spectroscopy (XPS), noncontact atomic force microscopy (nc-AFM), and density functional theory (DFT)-based computations to show that highly stable HO–H2O dimer species form at the (11̅02) facet of hematite; a promising anode material for photoelectrochemical water splitting. The UHV-based results are complemented by measurements following exposure to liquid water and are consistent with prior X-ray scattering results. The presence of strongly bound water agglomerates is generally not taken into account in OER reaction schemes but may play a role in determining the required OER overpotential on metal oxides.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b02324

Chinese Library Classification Number:

Citation Information:

The oxygen evolution reaction (OER) is thought to occur via a four-step mechanism with *O, *OH, and *OOH as adsorbed intermediates. Linear scaling of the *OH and **OOH adsorption energies is proposed to limit the oxides’ efficiency as OER catalysts, but the use of simple descriptors to screen candidate materials neglects potentially important water–water interactions. Here, we use a combination of temperature-programmed desorption (TPD), X-ray photoemission spectroscopy (XPS), noncontact atomic force microscopy (nc-AFM), and density functional theory (DFT)-based computations to show that highly stable HO–H2O dimer species form at the (11̅02) facet of hematite; a promising anode material for photoelectrochemical water splitting. The UHV-based results are complemented by measurements following exposure to liquid water and are consistent with prior X-ray scattering results. The presence of strongly bound water agglomerates is generally not taken into account in OER reaction schemes but may play a role in determining the required OER overpotential on metal oxides.

quote

GB/T 7714-2015 [1] Zdenek Jakub, Florian Kraushofer, Magdalena Bichler, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b02324.
MLA [1] Zdenek Jakub, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b02324.
APA [1] Zdenek Jakub, Florian Kraushofer, Magdalena Bichler, Jan Balajka, Jan Hulva, Jiri Pavelec, Igor Sokolović, Matthias Müllner, Martin Setvin, Michael Schmid, Ulrike Diebold, Peter Blaha, & Gareth S. Parkinson. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b02324
IEEE [1] Zdenek Jakub, Florian Kraushofer, Magdalena Bichler, Jan Balajka, Jan Hulva, Jiri Pavelec, Igor Sokolović, Matthias Müllner, Martin Setvin, Michael Schmid, Ulrike Diebold, Peter Blaha, and Gareth S. Parkinson, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b02324.