Facile preparation of vaterite dominated incineration fly ash (IFA) by slurry carbonation and its performance as supplementary cementitious material AITranslate

Taizhou University; Hunan University; Taizhou University; Taizhou University; Taizhou University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • Slurry carbonation on MSWIFA is sequentially optimized to precipitate more vaterite during treatment. • Vaterite precipitation is favored at lower temperature and higher water-ash ratio condition. • Vaterite dominated IFA has better performance than calcite CaCO3 as SCM. • Additional aluminate is preferred to promote reaction from vaterite to hemicarbonate in the cement paste. Municipal solid waste incineration fly ash (IFA) can be treated by slurry carbonation and adopted as a supplementary cementitious material (SCM) to reduce the carbon emission of the cement industry. However, effects of control parameters of carbonation on the mineralogy and morphology of the treated IFA require further investigation. In this work, the control parameters were sequentially optimized, aiming at producing more chemically active vaterite during carbonation. The vaterite dominated IFA was subsequently used as an SCM and its performance was studied and compared with limestone (pure calcite). Results indicated that precipitation of vaterite was favored under lower temperature and higher water-ash ratio conditions. CO2 flow rate has relatively smaller impact on the mineralogy of the treated IFA, but a higher rate led to agglomeration of vaterite particles. Under the optimized condition, vaterite dominated IFA containing 60% vaterite and 10% calcite was obtained. For the blended cement, its early hydration was suppressed by calcium sulfite (CaSO3) in the IFA, but the additional sulfate (CaSO4) accelerated the ettringite formation. The vaterite calcium carbonate in the treated IFA stabilized ettringite and reacted with aluminate phases to form hemicarbonate, refining the pore structure. However, hemicarbonate formation was limited by availability of aluminum that was consumed to form ettringite. Compared to limestone, the vaterite dominated IFA behaved better performance as an SCM, and the Porland cement can be substituted by 20% without compromising the 3-day and 28-day compressive strength. Toxicity leaching tests indicated only Pb exceeded regulatory limits in raw IFA, while Pb leaching in mortar samples was greatly declined below 1% of the limit.

KeyWords AITranslate

Municipal solid waste incineration fly ash Carbonation Vaterite Supplementary cementitious material Heavy metal leaching
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2023.e02775

Chinese Library Classification Number:

Citation Information:

Highlights • Slurry carbonation on MSWIFA is sequentially optimized to precipitate more vaterite during treatment. • Vaterite precipitation is favored at lower temperature and higher water-ash ratio condition. • Vaterite dominated IFA has better performance than calcite CaCO3 as SCM. • Additional aluminate is preferred to promote reaction from vaterite to hemicarbonate in the cement paste. Municipal solid waste incineration fly ash (IFA) can be treated by slurry carbonation and adopted as a supplementary cementitious material (SCM) to reduce the carbon emission of the cement industry. However, effects of control parameters of carbonation on the mineralogy and morphology of the treated IFA require further investigation. In this work, the control parameters were sequentially optimized, aiming at producing more chemically active vaterite during carbonation. The vaterite dominated IFA was subsequently used as an SCM and its performance was studied and compared with limestone (pure calcite). Results indicated that precipitation of vaterite was favored under lower temperature and higher water-ash ratio conditions. CO2 flow rate has relatively smaller impact on the mineralogy of the treated IFA, but a higher rate led to agglomeration of vaterite particles. Under the optimized condition, vaterite dominated IFA containing 60% vaterite and 10% calcite was obtained. For the blended cement, its early hydration was suppressed by calcium sulfite (CaSO3) in the IFA, but the additional sulfate (CaSO4) accelerated the ettringite formation. The vaterite calcium carbonate in the treated IFA stabilized ettringite and reacted with aluminate phases to form hemicarbonate, refining the pore structure. However, hemicarbonate formation was limited by availability of aluminum that was consumed to form ettringite. Compared to limestone, the vaterite dominated IFA behaved better performance as an SCM, and the Porland cement can be substituted by 20% without compromising the 3-day and 28-day compressive strength. Toxicity leaching tests indicated only Pb exceeded regulatory limits in raw IFA, while Pb leaching in mortar samples was greatly declined below 1% of the limit.

quote

GB/T 7714-2015 [1] Haijie He, Pengfei Ren, Junding Liu, et al. Case Studies in Construction Materials, 2024(20). DOI:10.1016/j.cscm.2023.e02775.
MLA [1] Haijie He, et al., Case Studies in Construction Materials, no. 20, 2024, https://doi.org/10.1016/j.cscm.2023.e02775.
APA [1] Haijie He, Pengfei Ren, Junding Liu, Ji Yuan, & Xinyu Shen. (2024). Case Studies in Construction Materials(20). https://doi.org/10.1016/j.cscm.2023.e02775
IEEE [1] Haijie He, Pengfei Ren, Junding Liu, Ji Yuan, and Xinyu Shen, Case Studies in Construction Materials, no. 20, 2024, doi: 10.1016/j.cscm.2023.e02775. keywords: {Municipal solid waste incineration fly ash;Carbonation;Vaterite;Supplementary cementitious material;Heavy metal leaching}