Improved Rate Capability in Composite Solid-State Battery Electrodes Using 3-D Architectures AITranslate

University of Michigan; University of Michigan; University of Michigan; University of Michigan
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The limited rate capability observed at faster charging rates is a critical challenge for composite electrodes in solid-state batteries (SSBs). This becomes further amplified with increasing electrode thickness and higher ratios of active material to solid electrode, which result in trade-offs between energy and power density. To overcome these trade-offs, it is necessary to understand the factors responsible for poor rate capability by exploring new approaches to boost power density without compromising energy density. Herein, we fabricated 3-D patterned composite graphite (Gr/Li6PS5Cl) electrodes with low-tortuosity electrolyte channels using a templating approach. Graphite was chosen as a model system to study inhomogeneous lithiation in composite SSB electrode architectures because of the visible color changes that occur as a function of local state-of-charge. At faster cycling rates (1C), the 3-D patterned electrodes enabled considerably higher accessible capacity (38% increase) compared to the unpatterned control electrodes. These enhancements were visualized using operando video microscopy, where 3-D electrode architectures showed improved homogeneity in the local state-of-charge throughout the electrode thickness. The insights presented here will enable new strategies based on 3-D electrode architectures to overcome power/energy trade-offs in SSBs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00528

Chinese Library Classification Number:

Citation Information:

The limited rate capability observed at faster charging rates is a critical challenge for composite electrodes in solid-state batteries (SSBs). This becomes further amplified with increasing electrode thickness and higher ratios of active material to solid electrode, which result in trade-offs between energy and power density. To overcome these trade-offs, it is necessary to understand the factors responsible for poor rate capability by exploring new approaches to boost power density without compromising energy density. Herein, we fabricated 3-D patterned composite graphite (Gr/Li6PS5Cl) electrodes with low-tortuosity electrolyte channels using a templating approach. Graphite was chosen as a model system to study inhomogeneous lithiation in composite SSB electrode architectures because of the visible color changes that occur as a function of local state-of-charge. At faster cycling rates (1C), the 3-D patterned electrodes enabled considerably higher accessible capacity (38% increase) compared to the unpatterned control electrodes. These enhancements were visualized using operando video microscopy, where 3-D electrode architectures showed improved homogeneity in the local state-of-charge throughout the electrode thickness. The insights presented here will enable new strategies based on 3-D electrode architectures to overcome power/energy trade-offs in SSBs.

quote

GB/T 7714-2015 [1] Manoj K. Jangid, Andrew L. Davis, Daniel W. Liao, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00528.
MLA [1] Manoj K. Jangid, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00528.
APA [1] Manoj K. Jangid, Andrew L. Davis, Daniel W. Liao, & Neil P. Dasgupta. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00528
IEEE [1] Manoj K. Jangid, Andrew L. Davis, Daniel W. Liao, and Neil P. Dasgupta, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00528.