Ring-Opening Copolymerization of α-Hydroxy-γ-butyrolactone and ε-Caprolactone. Toward the Metal-Free Synthesis of Functional Polyesters AITranslate
Abstract AITranslate
Organocatalysis has been widely developed over the past decades as an alternative to metal-based catalysis. The actual concerns have also promoted the development of sustainable and degradable polymers. In this context, γ-lactones are an interesting class of monomers that count many bio-based monomers, yielding polyesters that can be readily depolymerized. Also, the use of functional substituted lactones such as the α-hydroxy-γ-butyrolactone (HBL) affords polyesters with pendant groups offering possible postmodification reactions. This article focuses on the ring-opening copolymerization (ROCP) of α-hydroxy-γ-butyrolactone (HBL) and ε-caprolactone (ε-CL) in the presence of phosphazene P4 base (tert-BuP4) as catalyst. The bulk copolymerization at high temperature (80 °C) yielded fast kinetics (5 min) and high monomer conversions (98% for ε-CL; 88% for HBL) and molar masses (14900 g/mol with Đ = 3.8). A kinetics study at 80 °C revealed a partial HBL depolymerization over time. This phenomenon induced changes in the microstructures of the copolymers. Similar high conversions and molar masses could be also achieved at room temperature for 6 h without any depolymerization. Various monomer feed ratios were also evaluated affording copolyesters with up to 31% of incorporated HBL. In addition, DFT calculations with respect to the HBL homopolymerization revealed similar activation energies between different possible reactions, which include ring-opening polymerization, branching, and backbiting reactions.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01303
Chinese Library Classification Number:
Citation Information:
Organocatalysis has been widely developed over the past decades as an alternative to metal-based catalysis. The actual concerns have also promoted the development of sustainable and degradable polymers. In this context, γ-lactones are an interesting class of monomers that count many bio-based monomers, yielding polyesters that can be readily depolymerized. Also, the use of functional substituted lactones such as the α-hydroxy-γ-butyrolactone (HBL) affords polyesters with pendant groups offering possible postmodification reactions. This article focuses on the ring-opening copolymerization (ROCP) of α-hydroxy-γ-butyrolactone (HBL) and ε-caprolactone (ε-CL) in the presence of phosphazene P4 base (tert-BuP4) as catalyst. The bulk copolymerization at high temperature (80 °C) yielded fast kinetics (5 min) and high monomer conversions (98% for ε-CL; 88% for HBL) and molar masses (14900 g/mol with Đ = 3.8). A kinetics study at 80 °C revealed a partial HBL depolymerization over time. This phenomenon induced changes in the microstructures of the copolymers. Similar high conversions and molar masses could be also achieved at room temperature for 6 h without any depolymerization. Various monomer feed ratios were also evaluated affording copolyesters with up to 31% of incorporated HBL. In addition, DFT calculations with respect to the HBL homopolymerization revealed similar activation energies between different possible reactions, which include ring-opening polymerization, branching, and backbiting reactions.
quote
| GB/T 7714-2015 | [1] Chloé Pascouau, Raphaël Méreau, Etienne Grau, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01303. |
| MLA | [1] Chloé Pascouau, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01303. |
| APA | [1] Chloé Pascouau, Raphaël Méreau, Etienne Grau, AnneLaure Wirotius, Stéphane Carlotti, Henri Cramail, & Frédéric Peruch. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01303 |
| IEEE | [1] Chloé Pascouau, Raphaël Méreau, Etienne Grau, AnneLaure Wirotius, Stéphane Carlotti, Henri Cramail, and Frédéric Peruch, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01303. keywords: {anionic ringopening (co)polymerization;organocatalysis;αhydroxyγbutyrolactone;functional polyesters;sustainable polymers} |