Release of Fragrances from Polymer Coatings Triggered by Contact with Sweat AITranslate

Vidyasirimedhi Institute of Science and Technology (VISTEC); Vidyasirimedhi Institute of Science and Technology (VISTEC); Vidyasirimedhi Institute of Science and Technology (VISTEC)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Fragrances are active compounds that suffer from the fact that fragrances are usually quickly volatile and hence display a limited use in daily life applications. To overcome this problem, the fragrances benzaldehyde and heptanal are conjugated to a monomer via a hydrazone linkage. The functional monomers are then reacted with a urethane acrylate by photopolymerization to yield thin polymer coatings. The release of fragrances from the coatings was measured by UV–visible spectroscopy and headspace gas chromatography–mass spectrometry techniques, showing sustained release in artificial sweat due to the slow kinetics of the hydrolysis of the hydrazone linkage. This simple strategy can be applied for the rapid preparation of coatings on contact with wet human skin in labeling applications.

KeyWords AITranslate

coating controlled release fragrance pHresponsive polymer conjugate
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02052

Chinese Library Classification Number:

Citation Information:

Fragrances are active compounds that suffer from the fact that fragrances are usually quickly volatile and hence display a limited use in daily life applications. To overcome this problem, the fragrances benzaldehyde and heptanal are conjugated to a monomer via a hydrazone linkage. The functional monomers are then reacted with a urethane acrylate by photopolymerization to yield thin polymer coatings. The release of fragrances from the coatings was measured by UV–visible spectroscopy and headspace gas chromatography–mass spectrometry techniques, showing sustained release in artificial sweat due to the slow kinetics of the hydrolysis of the hydrazone linkage. This simple strategy can be applied for the rapid preparation of coatings on contact with wet human skin in labeling applications.

quote

GB/T 7714-2015 [1] Piangtawan Phoungtawee, Wimalin Jaroonwatana, Daniel Crespy. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02052.
MLA [1] Piangtawan Phoungtawee, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02052.
APA [1] Piangtawan Phoungtawee, Wimalin Jaroonwatana, & Daniel Crespy. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02052
IEEE [1] Piangtawan Phoungtawee, Wimalin Jaroonwatana, and Daniel Crespy, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02052. keywords: {coating;controlled release;fragrance;pHresponsive;polymer conjugate}