The present work deals with the synthesis and characterization of fluorescent polypropylene materials as well as the study of some properties, with the purpose of exploring their potential as specialty materials in high-thermal stability dielectrics. Direct copolymerization of propylene with 9-(undec-10-en-1-yl)-9H-carbazole, via metallocene catalysis, has allowed the preparation of materials containing up to 4 mol % of carbazole units. Characterization of obtained materials has shown that, besides fluorescence emission, improvements in both dielectric response and stability are important enough for potential use in PP-based film capacitors. In addition, an exploratory study on a UV-irradiated copolymer reveals that cross-linking between carbazole units is the mechanism that enables further improvements in thermal and thermo-oxidative stabilities, with respect to polypropylene.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01208
Chinese Library Classification Number:
Citation Information:
The present work deals with the synthesis and characterization of fluorescent polypropylene materials as well as the study of some properties, with the purpose of exploring their potential as specialty materials in high-thermal stability dielectrics. Direct copolymerization of propylene with 9-(undec-10-en-1-yl)-9H-carbazole, via metallocene catalysis, has allowed the preparation of materials containing up to 4 mol % of carbazole units. Characterization of obtained materials has shown that, besides fluorescence emission, improvements in both dielectric response and stability are important enough for potential use in PP-based film capacitors. In addition, an exploratory study on a UV-irradiated copolymer reveals that cross-linking between carbazole units is the mechanism that enables further improvements in thermal and thermo-oxidative stabilities, with respect to polypropylene.
quote
| GB/T 7714-2015 | [1] Daniel PlazaGonzález, Enrique BlázquezBlázquez, José Manuel GómezElvira, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01208. |
| MLA | [1] Daniel PlazaGonzález, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01208. |
| APA | [1] Daniel PlazaGonzález, Enrique BlázquezBlázquez, José Manuel GómezElvira, & Mario Hoyos. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01208 |
| IEEE | [1] Daniel PlazaGonzález, Enrique BlázquezBlázquez, José Manuel GómezElvira, and Mario Hoyos, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01208. keywords: {Functional polyolefins;photoactive polypropylene;crosslinked polypropylene;highthermal stability polypropylene;Show More} |