Toward Effective and Adsorption-Based Antifouling Zipper Brushes: Effect of pH, Salt, and Polymer Design AITranslate
Abstract AITranslate
The undesired spontaneous deposition and accumulation of matter on surfaces, better known as fouling, is a problematic and often inevitable process plaguing a variety of industries. This detrimental process can be reduced or even prevented by coating surfaces with a dense layer of end-grafted polymer: a polymer brush. Producing such polymer brushes via adsorption presents a very attractive technique, as large surfaces can be coated in a quick and simple manner. Recently, we introduced a simple and scalable two-step adsorption strategy to fabricate block copolymer-based antifouling coatings on hydrophobic surfaces. This two-step approach involved the initial adsorption of hydrophobic-charged diblock copolymer micelles acting as a primer, followed by the complexation of oppositely charged-antifouling diblock copolymers to form the antifouling brush coating. Here, we significantly improve this adsorption-based zipper brush via systematic tuning of various parameters, including pH, salt concentration, and polymer design. This study reveals several key outcomes. First of all, increasing the hydrophobic/hydrophilic block ratio of the anchoring polymeric micelles (i.e., decreasing the hydrophilic corona) promotes adsorption to the surface, resulting in the most densely packed, uniform, and hydrophilic primer layers. Second, around a neutral pH and at a low salt concentration (1 mM), complexation of the weak polyelectrolyte (PE) blocks results in brushes with the best antifouling efficacy. Moreover, by tuning the ratio between these PE blocks, the brush density can be increased, which is also directly correlated to the antifouling performance. Finally, switching to different antifouling blocks can increase the internal density or strengthen the bound hydration layer of the brush, leading to an additional enhancement of the antifouling properties (>99% lysozyme, 87% bovine serum albumin).
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01217
Chinese Library Classification Number:
Citation Information:
The undesired spontaneous deposition and accumulation of matter on surfaces, better known as fouling, is a problematic and often inevitable process plaguing a variety of industries. This detrimental process can be reduced or even prevented by coating surfaces with a dense layer of end-grafted polymer: a polymer brush. Producing such polymer brushes via adsorption presents a very attractive technique, as large surfaces can be coated in a quick and simple manner. Recently, we introduced a simple and scalable two-step adsorption strategy to fabricate block copolymer-based antifouling coatings on hydrophobic surfaces. This two-step approach involved the initial adsorption of hydrophobic-charged diblock copolymer micelles acting as a primer, followed by the complexation of oppositely charged-antifouling diblock copolymers to form the antifouling brush coating. Here, we significantly improve this adsorption-based zipper brush via systematic tuning of various parameters, including pH, salt concentration, and polymer design. This study reveals several key outcomes. First of all, increasing the hydrophobic/hydrophilic block ratio of the anchoring polymeric micelles (i.e., decreasing the hydrophilic corona) promotes adsorption to the surface, resulting in the most densely packed, uniform, and hydrophilic primer layers. Second, around a neutral pH and at a low salt concentration (1 mM), complexation of the weak polyelectrolyte (PE) blocks results in brushes with the best antifouling efficacy. Moreover, by tuning the ratio between these PE blocks, the brush density can be increased, which is also directly correlated to the antifouling performance. Finally, switching to different antifouling blocks can increase the internal density or strengthen the bound hydration layer of the brush, leading to an additional enhancement of the antifouling properties (>99% lysozyme, 87% bovine serum albumin).
quote
| GB/T 7714-2015 | [1] Anna M. C. Maan, Anton H. Hofman, Théophile Pelras, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01217. |
| MLA | [1] Anna M. C. Maan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01217. |
| APA | [1] Anna M. C. Maan, Anton H. Hofman, Théophile Pelras, Ilan M. Ruhof, Marleen Kamperman, & Wiebe M. de Vos. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01217 |
| IEEE | [1] Anna M. C. Maan, Anton H. Hofman, Théophile Pelras, Ilan M. Ruhof, Marleen Kamperman, and Wiebe M. de Vos, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01217. keywords: {antifouling coating;twostep adsorption;polymer brush;diblock copolymers;hydrophobic surfaces} |