daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Manipulation of Solubility and Interstitial Defects for Improving Thermoelectric SnTe Alloys AITranslate

Tongji University; Tongji University; Tongji University; Tongji University; Tongji University; The University of Hong Kong; Tongji University; The University of Hong Kong; Tongji University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Much effort has recently been directed at advancing thermoelectric SnTe as an alternative to PbTe. Effective methods include energy band convergence, nanostructures, and substitutional and interstitial defects. Among these strategies, it is shown that CdTe alloying effectively reduces the energy offset between valence bands for an enhanced thermoelectric figure of merit, zT. However, its solubility of only ∼6% might limit this effect on a full zT optimization in SnTe–CdTe alloys. Here, we show an effective approach for increasing CdTe solubility up to ∼20%, with the help of the existence of 5% GeTe. This leads the valence bands to be further converged for improving electronic performance. In addition, Cu2Te alloying is used to create interstitial defects for reducing the lattice thermal conductivity. Eventually, the increase of CdTe solubility and the creation of Cu interstitials enable a significantly enhanced zT, indicating the importance of solubility manipulation for engineering the band structure in thermoelectric SnTe alloys.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01098

Chinese Library Classification Number:

Citation Information:

Much effort has recently been directed at advancing thermoelectric SnTe as an alternative to PbTe. Effective methods include energy band convergence, nanostructures, and substitutional and interstitial defects. Among these strategies, it is shown that CdTe alloying effectively reduces the energy offset between valence bands for an enhanced thermoelectric figure of merit, zT. However, its solubility of only ∼6% might limit this effect on a full zT optimization in SnTe–CdTe alloys. Here, we show an effective approach for increasing CdTe solubility up to ∼20%, with the help of the existence of 5% GeTe. This leads the valence bands to be further converged for improving electronic performance. In addition, Cu2Te alloying is used to create interstitial defects for reducing the lattice thermal conductivity. Eventually, the increase of CdTe solubility and the creation of Cu interstitials enable a significantly enhanced zT, indicating the importance of solubility manipulation for engineering the band structure in thermoelectric SnTe alloys.

quote

GB/T 7714-2015 [1] Jing Tang, Bo Gao, Siqi Lin, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01098.
MLA [1] Jing Tang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01098.
APA [1] Jing Tang, Bo Gao, Siqi Lin, Xiao Wang, Xinyue Zhang, Fen Xiong, Wen Li, Yue Chen, & Yanzhong Pei. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01098
IEEE [1] Jing Tang, Bo Gao, Siqi Lin, Xiao Wang, Xinyue Zhang, Fen Xiong, Wen Li, Yue Chen, and Yanzhong Pei, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01098.