daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Hydrogen Spillover Intensified by Pt Sites on Single-Crystalline MoO3 Interconnected Branches for Hydrogen Evolution AITranslate

Queensland University of Technology; Shaanxi University of Science and Technology; Queensland University of Technology; Queensland University of Technology; Queensland University of Technology; Queensland University of Technology; Queensland University of Technology; Queensland University of Technology; Queensland University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hydrogen spillover is a well-recognized phenomenon in the electrocatalytic hydrogen evolution reaction (HER), and the spillover rate is highly dependent on metal–support interfaces. However, for the commonly used platinum (Pt) in HER, rational selection of the ideal support for intensifying spillover remains elusive. Herein, three-dimensional single-crystalline molybdenum oxide (s-MoO3) is proposed as an ideal support for active Pt sites. In contrast to these traditional support materials, the resultant s-MoO3 manifests an interconnected branch-like morphology, a zigzag-type stepped edge, a porous surface, and a partially reductive surface. By virtue of these morphological and structural advantages of s-MoO3 interconnected branches, the subsequent loading of Pt particles could induce the intensified spillover rate accompanied by the formation of the H(O)xMoO3 intermediate and thus the enhanced activity for HER. It is expected that this work will enrich the current knowledge on hydrogen spillover mechanisms and offer an effective intensification strategy for support-type catalysts.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01459

Chinese Library Classification Number:

Citation Information:

Hydrogen spillover is a well-recognized phenomenon in the electrocatalytic hydrogen evolution reaction (HER), and the spillover rate is highly dependent on metal–support interfaces. However, for the commonly used platinum (Pt) in HER, rational selection of the ideal support for intensifying spillover remains elusive. Herein, three-dimensional single-crystalline molybdenum oxide (s-MoO3) is proposed as an ideal support for active Pt sites. In contrast to these traditional support materials, the resultant s-MoO3 manifests an interconnected branch-like morphology, a zigzag-type stepped edge, a porous surface, and a partially reductive surface. By virtue of these morphological and structural advantages of s-MoO3 interconnected branches, the subsequent loading of Pt particles could induce the intensified spillover rate accompanied by the formation of the H(O)xMoO3 intermediate and thus the enhanced activity for HER. It is expected that this work will enrich the current knowledge on hydrogen spillover mechanisms and offer an effective intensification strategy for support-type catalysts.

quote

GB/T 7714-2015 [1] Juan Bai, Jing Shang, Jun Mei, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01459.
MLA [1] Juan Bai, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01459.
APA [1] Juan Bai, Jing Shang, Jun Mei, Xiaodong Wang, Chao Zhang, Hashara Kandambige, DongChen Qi, Ting Liao, & Ziqi Sun. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01459