daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Resolving the Hydrophobicity of the Me-4PACz Hole Transport Layer for Inverted Perovskite Solar Cells with Efficiency >20% AITranslate

Indian Institute of Technology Bombay;Helmholtz Young Investigator Group FRONTRUNNER; Indian Institute of Technology Bombay;IEK-5 Photovoltaik, Forschungszentrum Jülich; University of Duisburg-Essen; University of Stuttgart; Indian Institute of Technology Bombay
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A [4-(3,6-dimethyl-9H-carbazol-9-yl)butyl]phosphonic acid (Me-4PACz) self-assembled monolayer (SAM) has been employed in perovskite devices demonstrating high efficiencies. However, a uniform perovskite layer does not form due to the hydrophobicity of Me-4PACz. Here, we tackle this challenge by adding a conjugated polyelectrolyte, poly(9,9-bis(3′-(N,N-dimethyl)-N-ethylammonium-propyl-2,7-fluorene)-alt-2,7-(9,9-dioctylfluorene)) dibromide (PFN-Br), to the Me-4PACz in a specific ratio, defined as Pz:PFN. With this mixing engineering strategy using Pz:PFN, the PFN-Br interaction with the A-site cation is confirmed via solution-state nuclear magnetic resonance studies. The narrow full widths at half-maxima of diffraction peaks and photoluminescence spectra of perovskite films reveal improved crystallization at the optimal mixing ratio of Pz:PFN. Interestingly, the mixing of PFN-Br additionally tunes the work function of the Me-4PACz and the built-in voltage in the solar cells. Devices employing the optimized Pz:PFN mixing ratio deliver an open-circuit voltage of 1.16 V and efficiency >20% for perovskites with a bandgap of 1.6 eV with high reproducibility and concomitant stability.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01385

Chinese Library Classification Number:

Citation Information:

A [4-(3,6-dimethyl-9H-carbazol-9-yl)butyl]phosphonic acid (Me-4PACz) self-assembled monolayer (SAM) has been employed in perovskite devices demonstrating high efficiencies. However, a uniform perovskite layer does not form due to the hydrophobicity of Me-4PACz. Here, we tackle this challenge by adding a conjugated polyelectrolyte, poly(9,9-bis(3′-(N,N-dimethyl)-N-ethylammonium-propyl-2,7-fluorene)-alt-2,7-(9,9-dioctylfluorene)) dibromide (PFN-Br), to the Me-4PACz in a specific ratio, defined as Pz:PFN. With this mixing engineering strategy using Pz:PFN, the PFN-Br interaction with the A-site cation is confirmed via solution-state nuclear magnetic resonance studies. The narrow full widths at half-maxima of diffraction peaks and photoluminescence spectra of perovskite films reveal improved crystallization at the optimal mixing ratio of Pz:PFN. Interestingly, the mixing of PFN-Br additionally tunes the work function of the Me-4PACz and the built-in voltage in the solar cells. Devices employing the optimized Pz:PFN mixing ratio deliver an open-circuit voltage of 1.16 V and efficiency >20% for perovskites with a bandgap of 1.6 eV with high reproducibility and concomitant stability.

quote

GB/T 7714-2015 [1] Kashimul Hossain, Ashish Kulkarni, Urvashi Bothra, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01385.
MLA [1] Kashimul Hossain, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01385.
APA [1] Kashimul Hossain, Ashish Kulkarni, Urvashi Bothra, Benjamin Klingebiel, Thomas Kirchartz, Michael Saliba, & Dinesh Kabra. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01385
IEEE [1] Kashimul Hossain, Ashish Kulkarni, Urvashi Bothra, Benjamin Klingebiel, Thomas Kirchartz, Michael Saliba, and Dinesh Kabra, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01385.