Abstract AITranslate

High-crystalline g-C3N4 nanosheets (HC−CN) with reduced structural defects have been constructed through Ni-foam-induced thermal condensation because Ni-foam not only serves as a template for deposition of the 2D g-C3N4 nanosheets with high surface area to prevent stacking of g-C3N4 nanosheets but also acts as a catalyst to promote the polymerization and crystallization of g-C3N4 via effective dehydrogenation of the −NH2 group. The obtained HC–CN exhibits superior photocatalytic performance for H2 evolution under visible light irradiation (λ > 400 nm), which significantly benefits from the prolonged lifetime of photogenerated charge carriers and the increase of the transfer path within 2D structures of high-crystalline g-C3N4 nanosheets.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b01328

Chinese Library Classification Number:

Citation Information:

High-crystalline g-C3N4 nanosheets (HC−CN) with reduced structural defects have been constructed through Ni-foam-induced thermal condensation because Ni-foam not only serves as a template for deposition of the 2D g-C3N4 nanosheets with high surface area to prevent stacking of g-C3N4 nanosheets but also acts as a catalyst to promote the polymerization and crystallization of g-C3N4 via effective dehydrogenation of the −NH2 group. The obtained HC–CN exhibits superior photocatalytic performance for H2 evolution under visible light irradiation (λ > 400 nm), which significantly benefits from the prolonged lifetime of photogenerated charge carriers and the increase of the transfer path within 2D structures of high-crystalline g-C3N4 nanosheets.

quote

GB/T 7714-2015 [1] Weinan Xing, Wenguang Tu, Zhonghui Han, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01328.
MLA [1] Weinan Xing, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01328.
APA [1] Weinan Xing, Wenguang Tu, Zhonghui Han, Yidong Hu, Qingqiang Meng, & Gang Chen. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01328
IEEE [1] Weinan Xing, Wenguang Tu, Zhonghui Han, Yidong Hu, Qingqiang Meng, and Gang Chen, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01328.