Transient Species Mediating Energy Transfer to Spin-Forbidden Mn d States in II–VI Semiconductor Quantum Dots AITranslate

New Chemistry Unit, Jawaharlal Nehru Centre for Advanced Scientific Research;New Chemistry Unit and School of Advanced Materials (SAMat), Jawaharlal Nehru Centre for Advanced Scientific Research;Dipartimento di Fisica, Politecnico di Milano;Dipartimento di Fisica, Politecnico di Milano;Dipartimento di Fisica, Politecnico di Milano;Dipartimento di Energia, Politecnico di Milano;Theoretical Sciences Unit, Jawaharlal Nehru Centre for Advanced Scientific Research;Theoretical Sciences Unit and School of Advanced Materials (SAMat), Jawaharlal Nehru Centre for Advanced Scientific Research;New Chemistry Unit, International Centre for Materials Science and School of Advanced Materials (SAMat)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The nature of the transient species leading to emission from the spin/orbital-forbidden Mn d–d transition in doped semiconductor quantum dots has intrigued scientists for a long time. This understanding is important in the quest for energy efficiency as the energy from the conduction band is transferred efficiently to Mn in the femtosecond time scale overcoming other nonradiative recombination pathways. In this work, we have shown the presence of the transient species using materials with band gaps in resonance with the energy of the Mn emission to understand the nature of the absorbing, transient, and emitting species. Detailed studies lead to the emergence of a transient Mn3+ state that is further corroborated with spin-dependent density functional theory calculations. This opens up a unique opportunity to realize a reversible photochemical reaction and high radiative efficiency in a semiconductor nanostructure by controlling the spin state of the magnetic ion by external illumination.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00064

Chinese Library Classification Number:

Citation Information:

The nature of the transient species leading to emission from the spin/orbital-forbidden Mn d–d transition in doped semiconductor quantum dots has intrigued scientists for a long time. This understanding is important in the quest for energy efficiency as the energy from the conduction band is transferred efficiently to Mn in the femtosecond time scale overcoming other nonradiative recombination pathways. In this work, we have shown the presence of the transient species using materials with band gaps in resonance with the energy of the Mn emission to understand the nature of the absorbing, transient, and emitting species. Detailed studies lead to the emergence of a transient Mn3+ state that is further corroborated with spin-dependent density functional theory calculations. This opens up a unique opportunity to realize a reversible photochemical reaction and high radiative efficiency in a semiconductor nanostructure by controlling the spin state of the magnetic ion by external illumination.

quote

GB/T 7714-2015 [1] Kushagra Gahlot, Pradeep K.R., Andrea Camellini, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00064.
MLA [1] Kushagra Gahlot, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00064.
APA [1] Kushagra Gahlot, Pradeep K.R., Andrea Camellini, Gianluca Sirigu, Giulio Cerullo, Margherita ZavelaniRossi, Anjali Singh, Umesh V. Waghmare, & Ranjani Viswanatha. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00064
IEEE [1] Kushagra Gahlot, Pradeep K.R., Andrea Camellini, Gianluca Sirigu, Giulio Cerullo, Margherita ZavelaniRossi, Anjali Singh, Umesh V. Waghmare, and Ranjani Viswanatha, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00064.