Slow Carrier Cooling in Hybrid Pb–Sn Halide Perovskites AITranslate

University of Cambridge; University of Cambridge; University of Oxford; University of Cambridge; University of Cambridge
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Low band gap perovskites, such as mixed Pb–Sn systems, are essential to make bottom cells in all perovskite tandem photovoltaics. However, currently the fundamental dynamics of carriers in these materials are not well explored. Here we use ultrafast broad-band pump–probe spectroscopy to probe the two-stage carrier cooling dynamics in CH3NH3Pb1–xSnxI3 perovskites and show that the cooling is slower than that in pure Pb systems. The first-stage of cooling is associated with Fröhlich interactions between carriers and metal–iodide bonds that slow down monotonically with increasing Sn content. The second-tage of cooling involves the decay of an optical phonon into acoustic phonons and is slowest for 60% Sn content due to an increasing gap between the optical and acoustical phonon branches. Our results provide first insights into carrier cooling dynamics in hybrid Pb–Sn halide perovskites and pave the way for further understanding of the fundamental nature of Fröhlich interactions and the decay of optical phonons in perovskite systems.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00251

Chinese Library Classification Number:

Citation Information:

Low band gap perovskites, such as mixed Pb–Sn systems, are essential to make bottom cells in all perovskite tandem photovoltaics. However, currently the fundamental dynamics of carriers in these materials are not well explored. Here we use ultrafast broad-band pump–probe spectroscopy to probe the two-stage carrier cooling dynamics in CH3NH3Pb1–xSnxI3 perovskites and show that the cooling is slower than that in pure Pb systems. The first-stage of cooling is associated with Fröhlich interactions between carriers and metal–iodide bonds that slow down monotonically with increasing Sn content. The second-tage of cooling involves the decay of an optical phonon into acoustic phonons and is slowest for 60% Sn content due to an increasing gap between the optical and acoustical phonon branches. Our results provide first insights into carrier cooling dynamics in hybrid Pb–Sn halide perovskites and pave the way for further understanding of the fundamental nature of Fröhlich interactions and the decay of optical phonons in perovskite systems.

quote

GB/T 7714-2015 [1] Sachin Dev Verma, Qifei Gu, Aditya Sadhanala, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00251.
MLA [1] Sachin Dev Verma, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00251.
APA [1] Sachin Dev Verma, Qifei Gu, Aditya Sadhanala, Vijay Venugopalan, & Akshay Rao. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00251
IEEE [1] Sachin Dev Verma, Qifei Gu, Aditya Sadhanala, Vijay Venugopalan, and Akshay Rao, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00251.