Charge Transport in Single NCM Cathode Active Material Particles for Lithium-Ion Batteries Studied under Well-Defined Contact Conditions AITranslate

Justus Liebig University Giessen; Justus Liebig University Giessen; Justus Liebig University Giessen; Karlsruher Institute of Technology; Karlsruher Institute of Technology; Karlsruher Institute of Technology; Justus Liebig University Giessen; Justus Liebig University Giessen; Justus Liebig University Giessen; Justus Liebig University Giessen
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We present a technique for systematically investigating electronic and ionic charge transport in single Li(Ni1/3Co1/3Mn1/3)O2 (NCM 111) secondary particles as a function of size. We perform electrochemical impedance spectroscopy employing ion-blocking electrodes. Micrometer-sized spherical particles are arranged in cylindrical particle traps on a patterned substrate. A specially designed electrochemical cell is used to contact and measure individual immobilized particles in a defined contact geometry. The obtained electronic and ionic resistances of the particles as a function of size are compared with model calculations based on a homogeneous sphere with finite contact areas. The modeling reveals that electronic transport mainly occurs in the bulk of the NCM 111 particles, whereas ionic transport takes place along the particle surface. The extracted material parameters are in good agreement with literature values, showing the reliability of our measurement technique and its potential for systematic studies on the single-particle level.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01579

Chinese Library Classification Number:

Citation Information:

We present a technique for systematically investigating electronic and ionic charge transport in single Li(Ni1/3Co1/3Mn1/3)O2 (NCM 111) secondary particles as a function of size. We perform electrochemical impedance spectroscopy employing ion-blocking electrodes. Micrometer-sized spherical particles are arranged in cylindrical particle traps on a patterned substrate. A specially designed electrochemical cell is used to contact and measure individual immobilized particles in a defined contact geometry. The obtained electronic and ionic resistances of the particles as a function of size are compared with model calculations based on a homogeneous sphere with finite contact areas. The modeling reveals that electronic transport mainly occurs in the bulk of the NCM 111 particles, whereas ionic transport takes place along the particle surface. The extracted material parameters are in good agreement with literature values, showing the reliability of our measurement technique and its potential for systematic studies on the single-particle level.

quote

GB/T 7714-2015 [1] Simon Burkhardt, Markus S. Friedrich, Janis K. Eckhardt, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01579.
MLA [1] Simon Burkhardt, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01579.
APA [1] Simon Burkhardt, Markus S. Friedrich, Janis K. Eckhardt, Amalia C. Wagner, Nicole Bohn, Joachim R. Binder, Limei Chen, Matthias T. Elm, Jürgen Janek, & Peter J. Klar. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01579
IEEE [1] Simon Burkhardt, Markus S. Friedrich, Janis K. Eckhardt, Amalia C. Wagner, Nicole Bohn, Joachim R. Binder, Limei Chen, Matthias T. Elm, Jürgen Janek, and Peter J. Klar, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01579.