Experimental investigation on the influence of microwave technology on the treatability and mechanical properties of Portuguese southern blue gum wood AITranslate

University of Coimbra (UC); University of Coimbra (UC);Federal University of São Carlos (UFSCar);University Beira Interior (UBI);Innovation and Competence Forest Centre (SerQ), Rua J
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • Eucalyptus globulus wood species has several technological benefits but has drying and treatability issues. • Microwave (MW) treatment of Portuguese eucalyptus could improve its usage by overcoming its low permeability issues. • After MW treatment, the eucalyptus specimens had a 130 % increase in the retention of the preservative product. • The studied mechanical properties of MW-treated eucalyptus samples had no statistically significant reductions. • Microwave treatment is a feasible technology for wood modification, especially for contributing to the wide use of eucalyptus. Despite presenting global relevance and satisfactory mechanical properties for structural applications, the Portuguese eucalyptus, southern blue gum (Eucalyptus globulus Labill.), faces difficulties with impregnation with preservative products due to its limited permeability (treatability), which limits its utilization. Microwave (MW) treatment of wood offers a promising avenue for overcoming this issue, but it may impact the mechanical properties. It was identified that there remain research gaps regarding the impacts of MW treatment on eucalyptus. Hence, it was aimed to identify the optimum MW parameters for southern blue gum wood to enhance its impregnability without compromising the mechanical properties. This will contribute to meeting the growing demand for wood for construction. Small clear wood specimens containing heartwood were separated into three groups: two underwent MW treatment, and one did not (control). The samples were impregnated with a preservative product and after submitted to mechanical testing. The MW treatment significantly enhanced the retention of the preservative product, which is remarkable given the impossibility of impregnating eucalyptus heartwood using conventional pressure methods. Although there were slight decreases in the mechanical properties of the MW-treated specimens, they were statistically equivalent to the control group. New insights into the mechanical bending behavior of MW-treated samples also arose. The mechanical properties of MW-treated eucalyptus samples surpassed those of other globally used wood species. Thus, MW treatment presented itself as an effective process for increasing eucalyptus impregnability, and it has the potential to augment southern blue gum`s use as a raw sawn and engineered structural wood material worldwide. Graphical Download : Download high-res image (286KB) Download : Download full-size image

KeyWords AITranslate

Microwave treatment Portuguese eucalyptus Treatability Preservative product Mechanical properties
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2023.e02698

Chinese Library Classification Number:

Citation Information:

Highlights • Eucalyptus globulus wood species has several technological benefits but has drying and treatability issues. • Microwave (MW) treatment of Portuguese eucalyptus could improve its usage by overcoming its low permeability issues. • After MW treatment, the eucalyptus specimens had a 130 % increase in the retention of the preservative product. • The studied mechanical properties of MW-treated eucalyptus samples had no statistically significant reductions. • Microwave treatment is a feasible technology for wood modification, especially for contributing to the wide use of eucalyptus. Despite presenting global relevance and satisfactory mechanical properties for structural applications, the Portuguese eucalyptus, southern blue gum (Eucalyptus globulus Labill.), faces difficulties with impregnation with preservative products due to its limited permeability (treatability), which limits its utilization. Microwave (MW) treatment of wood offers a promising avenue for overcoming this issue, but it may impact the mechanical properties. It was identified that there remain research gaps regarding the impacts of MW treatment on eucalyptus. Hence, it was aimed to identify the optimum MW parameters for southern blue gum wood to enhance its impregnability without compromising the mechanical properties. This will contribute to meeting the growing demand for wood for construction. Small clear wood specimens containing heartwood were separated into three groups: two underwent MW treatment, and one did not (control). The samples were impregnated with a preservative product and after submitted to mechanical testing. The MW treatment significantly enhanced the retention of the preservative product, which is remarkable given the impossibility of impregnating eucalyptus heartwood using conventional pressure methods. Although there were slight decreases in the mechanical properties of the MW-treated specimens, they were statistically equivalent to the control group. New insights into the mechanical bending behavior of MW-treated samples also arose. The mechanical properties of MW-treated eucalyptus samples surpassed those of other globally used wood species. Thus, MW treatment presented itself as an effective process for increasing eucalyptus impregnability, and it has the potential to augment southern blue gum`s use as a raw sawn and engineered structural wood material worldwide. Graphical Download : Download high-res image (286KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Fernando J.R. Mascarenhas, Alfredo M.P.G. Dias, André L. Christoforo, et al. Case Studies in Construction Materials, 2024(20). DOI:10.1016/j.cscm.2023.e02698.
MLA [1] Fernando J.R. Mascarenhas, et al., Case Studies in Construction Materials, no. 20, 2024, https://doi.org/10.1016/j.cscm.2023.e02698.
APA [1] Fernando J.R. Mascarenhas, Alfredo M.P.G. Dias, André L. Christoforo, Rogério M.S. Simões, & André M.A. Dias. (2024). Case Studies in Construction Materials(20). https://doi.org/10.1016/j.cscm.2023.e02698
IEEE [1] Fernando J.R. Mascarenhas, Alfredo M.P.G. Dias, André L. Christoforo, Rogério M.S. Simões, and André M.A. Dias, Case Studies in Construction Materials, no. 20, 2024, doi: 10.1016/j.cscm.2023.e02698. keywords: {Microwave treatment;Portuguese eucalyptus;Treatability;Preservative product;Mechanical properties}