Photovoltaic Performance of FAPbI3 Perovskite Is Hampered by Intrinsic Quantum Confinement AITranslate
Abstract AITranslate
Formamidinium lead trioiodide (FAPbI3) is a promising perovskite for single-junction solar cells. However, FAPbI3 is metastable at room temperature and can cause intrinsic quantum confinement effects apparent through a series of above-bandgap absorption peaks. Here, we explore three common solution-based film-fabrication methods, neat N,N-dimethylformamide (DMF)–dimethyl sulfoxide (DMSO) solvent, DMF-DMSO with methylammonium chloride, and a sequential deposition approach. The latter two offer enhanced nucleation and crystallization control and suppress such quantum confinement effects. We show that elimination of these absorption features yields increased power conversion efficiencies (PCEs) and short-circuit currents, suggesting that quantum confinement hinders charge extraction. A meta-analysis of literature reports, covering 244 articles and 825 photovoltaic devices incorporating FAPbI3 films corroborates our findings, indicating that PCEs rarely exceed a 20% threshold when such absorption features are present. Accordingly, ensuring the absence of these absorption features should be the first assessment when designing fabrication approaches for high-efficiency FAPbI3 solar cells.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00656
Chinese Library Classification Number:
Citation Information:
Formamidinium lead trioiodide (FAPbI3) is a promising perovskite for single-junction solar cells. However, FAPbI3 is metastable at room temperature and can cause intrinsic quantum confinement effects apparent through a series of above-bandgap absorption peaks. Here, we explore three common solution-based film-fabrication methods, neat N,N-dimethylformamide (DMF)–dimethyl sulfoxide (DMSO) solvent, DMF-DMSO with methylammonium chloride, and a sequential deposition approach. The latter two offer enhanced nucleation and crystallization control and suppress such quantum confinement effects. We show that elimination of these absorption features yields increased power conversion efficiencies (PCEs) and short-circuit currents, suggesting that quantum confinement hinders charge extraction. A meta-analysis of literature reports, covering 244 articles and 825 photovoltaic devices incorporating FAPbI3 films corroborates our findings, indicating that PCEs rarely exceed a 20% threshold when such absorption features are present. Accordingly, ensuring the absence of these absorption features should be the first assessment when designing fabrication approaches for high-efficiency FAPbI3 solar cells.
quote
| GB/T 7714-2015 | [1] Karim A. Elmestekawy, Benjamin M. Gallant, Adam D. Wright, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00656. |
| MLA | [1] Karim A. Elmestekawy, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00656. |
| APA | [1] Karim A. Elmestekawy, Benjamin M. Gallant, Adam D. Wright, Philippe Holzhey, Nakita K. Noel, Michael B. Johnston, Henry J. Snaith, & Laura M. Herz. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00656 |
| IEEE | [1] Karim A. Elmestekawy, Benjamin M. Gallant, Adam D. Wright, Philippe Holzhey, Nakita K. Noel, Michael B. Johnston, Henry J. Snaith, and Laura M. Herz, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00656. |