Durability assessment of mechanochemically activated geopolymer concrete with a low molarity alkali solution AITranslate

Indian Institute of Technology;University Institute of Technology;Department of Civil Engineering, JSPM Nahre Technical Campus; Council of Scientific and Industrial Research -Advanced Materials and Processes Research Institute; Council of Scientific and Industrial Research -Advanced Materials and Processes Research Institute; Indian Institute of Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • Mechanochemically activated solely GGBS-based geopolymer concrete (GC) is prepared. • Two concentrations of alkali solution, i.e., 2 M and 12 M are used to prepare GC. • GC’s durability properties are compared with Portland slag cement concrete (PC). • GC exhibited better durability due to forming a dense matrix as compared to PC. • GC of a 2 M alkali concentration is found more sustainable than a 12 M concentration mix. The prevailing practices of geopolymer concrete (GC) preparation use a high concentration of alkali activators, which is uneconomical. It is imperative to develop GC of low-concentration activators with enhanced durability for field implementation. Mechanochemical activation of geopolymer increases the reactivity of its raw materials by converting the crystalline phase to an amorphous phase. It has been illustrated in the present study that mechanochemical activation aids in achieving GC of desired properties at low concentrations of alkali activators. The mechanochemical activation of ground granulated blast furnace slag (GGBS) with sodium metasilicate was carried out to prepare GC of low (2 M) and high (12 M) alkali concentrations. The Portland slag cement-based concrete (PC) was cast to compare the durability performance of GC. The durability of the three concrete mixes was examined in terms of water absorption, the volume of permeable voids (VPV), water and chloride permeability, homogeneity, and acid resistance. The microstructural characterization of concrete samples exposed to acid were carried out by X-ray diffraction, field emission scanning electron microscope, and energy dispersive X-ray spectrometer. The results indicated that GC with a low concentration of activator exhibited lesser water absorption, VPV, and permeability, whereas it offered higher resistance to acids and chloride ion penetrability. Low-concentration GC had a dense and compact structure due to the coexistence of geopolymeric and hydration products, leading to better performance than high-concentration GC and PC. The evaluation of cost and carbon emission of PC, and GC mixes suggests GC as a sustainable alternative to traditional concrete. Although PC is economically viable, the study suggest use of GC with low alkali concentration due to its environmental benefits with a minor increase in cost.

KeyWords AITranslate

Geopolymer Mechanochemical activation Portland slag cementbased concrete Durability Acid attack
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2023.e02715

Chinese Library Classification Number:

Citation Information:

Highlights • Mechanochemically activated solely GGBS-based geopolymer concrete (GC) is prepared. • Two concentrations of alkali solution, i.e., 2 M and 12 M are used to prepare GC. • GC’s durability properties are compared with Portland slag cement concrete (PC). • GC exhibited better durability due to forming a dense matrix as compared to PC. • GC of a 2 M alkali concentration is found more sustainable than a 12 M concentration mix. The prevailing practices of geopolymer concrete (GC) preparation use a high concentration of alkali activators, which is uneconomical. It is imperative to develop GC of low-concentration activators with enhanced durability for field implementation. Mechanochemical activation of geopolymer increases the reactivity of its raw materials by converting the crystalline phase to an amorphous phase. It has been illustrated in the present study that mechanochemical activation aids in achieving GC of desired properties at low concentrations of alkali activators. The mechanochemical activation of ground granulated blast furnace slag (GGBS) with sodium metasilicate was carried out to prepare GC of low (2 M) and high (12 M) alkali concentrations. The Portland slag cement-based concrete (PC) was cast to compare the durability performance of GC. The durability of the three concrete mixes was examined in terms of water absorption, the volume of permeable voids (VPV), water and chloride permeability, homogeneity, and acid resistance. The microstructural characterization of concrete samples exposed to acid were carried out by X-ray diffraction, field emission scanning electron microscope, and energy dispersive X-ray spectrometer. The results indicated that GC with a low concentration of activator exhibited lesser water absorption, VPV, and permeability, whereas it offered higher resistance to acids and chloride ion penetrability. Low-concentration GC had a dense and compact structure due to the coexistence of geopolymeric and hydration products, leading to better performance than high-concentration GC and PC. The evaluation of cost and carbon emission of PC, and GC mixes suggests GC as a sustainable alternative to traditional concrete. Although PC is economically viable, the study suggest use of GC with low alkali concentration due to its environmental benefits with a minor increase in cost.

quote

GB/T 7714-2015 [1] Ashita Singh, Sudhir Singh Bhadauria, Akshay Anil Thakare, et al. Case Studies in Construction Materials, 2024(20). DOI:10.1016/j.cscm.2023.e02715.
MLA [1] Ashita Singh, et al., Case Studies in Construction Materials, no. 20, 2024, https://doi.org/10.1016/j.cscm.2023.e02715.
APA [1] Ashita Singh, Sudhir Singh Bhadauria, Akshay Anil Thakare, Anil Kumar, Manish Mudgal, & Sandeep Chaudhary. (2024). Case Studies in Construction Materials(20). https://doi.org/10.1016/j.cscm.2023.e02715
IEEE [1] Ashita Singh, Sudhir Singh Bhadauria, Akshay Anil Thakare, Anil Kumar, Manish Mudgal, and Sandeep Chaudhary, Case Studies in Construction Materials, no. 20, 2024, doi: 10.1016/j.cscm.2023.e02715. keywords: {Geopolymer;Mechanochemical activation;Portland slag cementbased concrete;Durability;Acid attack}