Experimental investigation of the dynamic mechanical properties of concrete under different strain rates and cyclic loading AITranslate

Hohai University; Hohai University;Power Construction Corporation of China, Beijing 100048; Hohai University; Hohai University; Hohai University; Hohai University; Hohai University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • Dynamic mechanical tests of concrete under different cyclic loads and strain rates. • Effects of cyclic loading and strain rate on mechanical parameters of concrete. • Quantitative relationships among concrete mechanical parameters, cyclic loading and strain rate. • Mechanisms of cyclic loading effects on mechanical parameters of concrete. To investigate the effects of strain rate and cyclic loading on the mechanical parameters of concrete compressive strength, residual strain, peak strain and elastic modulus, a series of cyclic loading tests over concrete were conducted by setting different numbers of cycles, magnitude factors, and cycle frequencies/periods based on the FST-1000 alpine geotechnical dynamic and static triaxial test system. The quantitative relationships between the mechanical parameters of concrete and the parameters of cyclic loading as well as the strain rate were also proposed. The results show that as the strain rate increases, the concrete compressive strength and elastic modulus increase linearly, while the residual strength and peak strain show a decreasing trend. Under cyclic loading, the compressive strength was quadratically related to each cyclic loading parameter, and the elastic modulus was quadratically related to the cyclic number and magnitude factor. The trend of the concrete compressive strength rate sensitivity undergoes a change at the specific thresholds of 0.145 for the magnitude factor and 1.93 Hz for the frequency. The minimum value of the peak strain rate sensitivity corresponds to the specific thresholds of 6023 for the number of cycles, 0.14 for the magnitude factor, and 1.38 Hz for the frequency thresholds, respectively. Additionally, the enhancement of the elastic modulus rate sensitivity occurs when the number of cycles exceeds 918 or when the magnitude factor surpasses 0.33. The results can provide a theoretical basis for the design of concrete structures and seismic engineering.

KeyWords AITranslate

Strain rate Cyclic loading Concrete Compressive strength Rate sensitivities
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2023.e02750

Chinese Library Classification Number:

Citation Information:

Highlights • Dynamic mechanical tests of concrete under different cyclic loads and strain rates. • Effects of cyclic loading and strain rate on mechanical parameters of concrete. • Quantitative relationships among concrete mechanical parameters, cyclic loading and strain rate. • Mechanisms of cyclic loading effects on mechanical parameters of concrete. To investigate the effects of strain rate and cyclic loading on the mechanical parameters of concrete compressive strength, residual strain, peak strain and elastic modulus, a series of cyclic loading tests over concrete were conducted by setting different numbers of cycles, magnitude factors, and cycle frequencies/periods based on the FST-1000 alpine geotechnical dynamic and static triaxial test system. The quantitative relationships between the mechanical parameters of concrete and the parameters of cyclic loading as well as the strain rate were also proposed. The results show that as the strain rate increases, the concrete compressive strength and elastic modulus increase linearly, while the residual strength and peak strain show a decreasing trend. Under cyclic loading, the compressive strength was quadratically related to each cyclic loading parameter, and the elastic modulus was quadratically related to the cyclic number and magnitude factor. The trend of the concrete compressive strength rate sensitivity undergoes a change at the specific thresholds of 0.145 for the magnitude factor and 1.93 Hz for the frequency. The minimum value of the peak strain rate sensitivity corresponds to the specific thresholds of 6023 for the number of cycles, 0.14 for the magnitude factor, and 1.38 Hz for the frequency thresholds, respectively. Additionally, the enhancement of the elastic modulus rate sensitivity occurs when the number of cycles exceeds 918 or when the magnitude factor surpasses 0.33. The results can provide a theoretical basis for the design of concrete structures and seismic engineering.

quote

GB/T 7714-2015 [1] Lei Gan, Yu Liu, Zongliang Zhang, et al. Case Studies in Construction Materials, 2024(20). DOI:10.1016/j.cscm.2023.e02750.
MLA [1] Lei Gan, et al., Case Studies in Construction Materials, no. 20, 2024, https://doi.org/10.1016/j.cscm.2023.e02750.
APA [1] Lei Gan, Yu Liu, Zongliang Zhang, Zhenzhong Shen, Lechen Li, Hongwei Zhang, Hongjie Jin, & Weichao Xu. (2024). Case Studies in Construction Materials(20). https://doi.org/10.1016/j.cscm.2023.e02750
IEEE [1] Lei Gan, Yu Liu, Zongliang Zhang, Zhenzhong Shen, Lechen Li, Hongwei Zhang, Hongjie Jin, and Weichao Xu, Case Studies in Construction Materials, no. 20, 2024, doi: 10.1016/j.cscm.2023.e02750. keywords: {Strain rate;Cyclic loading;Concrete;Compressive strength;Rate sensitivities}